Polar-group-containing cyclized rubber and process for producing same
Abstract
A main object of the invention is to provide a polar-group-containing cyclized rubber making it possible to improve remarkable the adhesiveness between paint and a molded product made of a nonpolar polymer such as polypropylene or polyethylene, and a process for producing the same. In order to attain the object, the invention provides a polar-group-containing cyclized rubber which has a polar group at a terminal of a polymer chain thereof, has a weight-average molecular weight of 1000 to 1,000,000, and is obtained by cyclizing a conjugated diene polymer having the polar group at a terminal of a polymer chain thereof.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 11.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing a polar-group-containing cyclized rubber, comprising: the steps of: using an organic active metal catalyst to polymerize a conjugated diene monomer, or a conjugated diene monomer and a monomer copolymerizable with the conjugated diene monomer to produce an active conjugated diene polymer having an active metal at a terminal of a polymer chain thereof; causing a polar-group-containing compound to react with the active conjugated diene polymer to produce a polar-group-containing conjugated diene polymer having, at a terminal of a polymer chain thereof, a polar group origi
- Claim 2Independent Claim
The process for producing a polar-group-containin
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (11 of 11 total)
References Cited — Backward Prior Art (10)
Non-Patent Literature (1)
- English Language translation of JP 57-145103; publication date: Sep. 8, 1982.