US 7,273,635 B2#27004077 Most CitedExpiredUnited States (USPTO)Utility

Method of forming aluminide diffusion coatings

4Forward Citations (#27004077 Global)
0.2/yrCitation Velocity (#32418714 Global)
1.12Citation PageRank (#35488373 Global)
32Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Method of forming an outwardly grown aluminide diffusion coating on a superalloy substrate disposed in a coating retort including the steps of heating the substrate to a temperature of 900 to 1200 degrees C., flowing a coating gas comprising aluminum trichloride and a carrier gas through the coating retort at a flow rate of the coating gas of about 100 to about 450 standard cubic feet per hour, providing a concentration of aluminum trichloride in the retort of less than 1.4% by volume of the coating gas, and providing a total pressure of the coating gas in the coating retort of about 100 to about 450 Torr.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of forming an outwardly grown aluminide diffusion coating on a superalloy substrate disposed in a coating chamber, comprising heating the substrate to a temperature of 900 to 1200 degrees C., flowing a coating gas mixture comprising aluminum trichloride and a carrier gas through the chamber at a flow rate of the coating gas of about 100 to about 450 standard cubic feet per hour, providing a concentration of aluminum trichloride of less than about 1.4% by volume of the coating gas mixture in the chamber, and providing a total pressure of the coating gas mixture in the chamber of about

  2. Claim 2Depends on #1

    The method of claim 1 wherein the flow rate of coating gas mixture through the chamber is 200 to 400 standard cubic feet per hour, the concentration of alum

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (32)

PatentTitleYearCitations
US 4,761,267 AAluminum alloy for use as core of clad material198825
US 4,977,036 ACoating and compositions199021
US 5,028,385 ATreatment of metals for coating or activation199127
US 5,124,006 AMethod of forming heat engine parts made of a superalloy and having a metallic-ceramic protective coating199221
EP 0,496,935 A1Aluminide processing of articles protected by a thermal barrier coating system—14
US 5,261,963 ACVD apparatus comprising exhaust gas condensation means199347
US 5,264,245 ACVD method for forming uniform coatings199360
US 5,407,704 ACVD apparatus and method199532
US 5,462,013 ACVD apparatus and method for forming uniform coatings199535
JP H08260147 AChemically vapor-deposited aluminide member of heat-resistant alloy and its formation—3
US 5,658,614 APlatinum aluminide CVD coating method1997112
US 5,716,720 AThermal barrier coating system with intermediate phase bondcoat1998163
US 5,788,823 APlatinum modified aluminide diffusion coating and method199863
US 5,789,089 AHot-dipped aluminum coated steel sheet having excellent corrosion resistance and heat resistance, and production method thereof199838
US 5,856,027 AThermal barrier coating system with intermediate phase bondcoat1999119
EP 0,933,448 A1Improved diffusion aluminide bond coat for a thermal barrier coating system and a method therefor—17
US 5,989,733 AActive element modified platinum aluminide diffusion coating and CVD coating method199964
US 6,074,602 AProperty-balanced nickel-base superalloys for producing single crystal articles200094
US 6,129,991 AAluminide/MCrAlY coating system for superalloys200079
US 6,136,451 APlatinum modified aluminide diffusion coating and method200017
US 6,143,361 AMethod of reacting excess CVD gas reactant200015
US 6,153,313 ANickel aluminide coating and coating systems formed therewith2000112
US 6,168,874 B1Diffusion aluminide bond coat for a thermal barrier coating system and method therefor200156
EP 1,079,073 A2Modified diffusion aluminide coating for internal surfaces of gas turbine components—22
US 6,258,461 B1Activated nickel screens and foils20019
US 6,273,678 B1Modified diffusion aluminide coating for internal surfaces of gas turbine components200165

Non-Patent Literature (2)

  • "Surface-Aluminizing of Pt With AlCl<SUB>3 </SUB>Vapor," Nanko et al., Electrochemical Society Proceedings, vol. 99, No. 38, 2000, pp. 236-246.
  • Conner et al.; "Evaluation of Simple Aluminide and Platinum Modified Aluminide Coatings on High Pressure Turbine Blades after Factory Engigne Testing", Proc. AMSE Int. Conf. of Gas Turbine and Aero Engine Congress Jun. 3-6, 1991, and Jun. 1-4, 1992. No page numbers.