Patents
US 7,267,808 B2#32350025 Most CitedExpiredUnited States (USPTO)Utility

Aluminum nitride powder, method for producing the same and use thereof

3Forward Citations (#32350025 Global)
0.2/yrCitation Velocity (#38171491 Global)
1.10Citation PageRank (#36422796 Global)
12Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention is to produce an aluminum nitride powder which is turned into a sintered body at a temperature of not more than 1600° C., thereby obtaining a sintered aluminum nitride in which the density and thermal conductivity are high and which can be properly used as a substrate material. Using a vapor phase reaction apparatus shown in FIG. 1 , ammonia gas was fed from a reactor 2 heated at from 300 to 500° C. and maintained at that temperature by a heating section 1 via a feeding tube 4 while being regulated by a flow regulator 3 . At the same time, while being regulated by the flow regulator 5 , nitrogen gas containing an organic aluminum compound is fed via a feeding tube 6 to obtain an aluminum nitride powder. The aluminum nitride powder is subjected to a heat treatment at from 1100 to 1500° C. in a reducing gas atmosphere and/or an inert gas atmosphere to obtain an aggregate aluminum nitride powder. The aggregate aluminum nitride powder is subjected to a mechanical treatment to obtain an aluminum nitride powder in which the specific surface area value is not less than 30 m 2 /g and a ratio of an average particle diameter to a particle diameter in terms of the specif

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An aluminum nitride powder, wherein a primary particle diameter is not more than 0.06 μm and a ratio of a secondary particle diameter to the primary particle diameter (a secondary particle diameter/a primary particle diameter) is not more than 10.

  2. Claim 2Depends on #1

    The aluminum nitride powder according to claim 1 , wherein the primary particle diameter is from 0.012 to 0.06 μm and a ratio of the secondary particle diameter to the primary particle diameter (a secondary particle diameter/a primary particle diameter) is from 1 to 10.

  3. Claim 3Depends on #1

    The aluminum nitride powder according to claim 1 , wherein the aluminum nitride powder is turned into a sintered body having a density of not less than 98% of a theoretical density by calcination under an atmospheric pressure and at a temperature of from 1400 to 1600° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Ceramics Japan, (32), No. 6 (3 pp), no date.