Method for continuous production of high-molecular weight polyesters and device for implementation of the method

10Forward Citations (#10348780 Global)
0.5/yrCitation Velocity (#14910180 Global)
2.21Citation PageRank (#12428513 Global)
1Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a method for producing high-molecular weight polyesters, such as e.g. polyethylene terephthalate (PET), polybutylene terephthalate (PBT), polynaphthalene terephthalate (PEN), polytrimethylene terephthalate (PTT) and/or polyesters of other dicarboxylic acids and diols including copolymers thereof. The invention relates likewise to a device for implementing this method. The latter concerns a single-stage tower reactor with which a method, comprising only two reactors, is made available for the total process.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A device for continuous production of high-molecular weight polyester by at least one of esterification of dicarboxylic acids and transesterification of dicarboxylic acid esters with diols in the presence of catalysts with formation of a prepolymer and polycondensation thereof into high-molecular weight polyester by at least one of a1) producing at least one of a paste and a suspension of the dicarboxylic acid and of the diol while maintaining a molar ratio of diol to dicarboxylic acid of 0.8 to 1.8, a temperature of 20 to 90° C. and a pressure between 0.1 to 1.0 bar, or a2) melting the dicarb