Method for forming aluminum interconnect

1Forward Citations (#60942087 Global)
0.1/yrCitation Velocity (#54862680 Global)
0.76Citation PageRank (#60942087 Global)
25Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for forming an Al interconnect is disclosed. A disclosed method comprises: depositing a Ti layer on a substrate having predetermined devices; depositing a TiN layer on the entire surface of the Ti layer by performing a CVD process; performing a plasma treatment for the TiN layer; depositing an Al layer on the TiN layer; and forming an ARC on the entire surface of the Al layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming an Al interconnect comprising the steps of: depositing a planar Ti layer on a substrate having a completely planar upper surface; depositing a planar TiN layer on an entire upper surface of the planar Ti layer by chemical vapor deposition (CVD), wherein the deposited TiN layer has a thickness less than 120 Å; plasma treating the TiN layer, wherein the plasma treated TiN layer has a thickness less than 60 Å; depositing an Al layer on an entire surface of the plasma treated TiN layer to form the Al interconnect; and forming an ARC on the entire surface of the Al layer.

  2. Claim 2Depends on #1

    A method as defined by claim 1 , wherein the plasma treated TiN layer has nano-crystallinity.

  3. Claim 3Depends on #1

    A method as defined by claim 1 , wherein the Al layer is deposited at a temperature between 300° C. and 450° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (25)

PatentTitleYearCitations
US 5,008,216 AProcess for improved contact stud structure for semiconductor devices199139
US 5,008,730 AContact stud structure for semiconductor devices199137
US 5,401,675 AMethod of depositing conductors in high aspect ratio apertures using a collimator199541
US 5,403,779 ARefractory metal capped low resistivity metal conductor lines and vias formed using PVD and CVD1995103
US 5,627,102 AMethod for making metal interconnection with chlorine plasma etch199777
US 5,760,475 ARefractory metal-titanium nitride conductive structures199854
US 5,889,328 ARefractory metal capped low resistivity metal conductor lines and vias199977
US 6,063,703 AMethod for making metal interconnection200049
US 6,069,072 ACVD tin barrier layer for reduced electromigration of aluminum plugs200029
US 6,110,828 AIn-situ capped aluminum plug (CAP) process using selective CVD AL for integrated plug/interconnect metallization200049
US 6,140,228 ALow temperature metallization process200047
US 6,169,327 B1Metal interconnection structure of semiconductor device20012
US 6,187,667 B1Method of forming metal layer(s) and/or antireflective coating layer(s) on an integrated circuit200116
US 6,200,895 B1Method of forming an electrical connection200126
KR 20010078086 APlasma-enhanced chemical vapor deposition of a metal nitride layer—4
US 6,309,971 B1Hot metallization process20015
US 6,333,261 B1Method for preventing aluminum intrusions200112
US 6,338,880 B1Chemical vapor deposition process for depositing titanium nitride films from an organometallic compound200228
JP 2002033322 AMethod of manufacturing semiconductor device—2
US 6,522,013 B1Punch-through via with conformal barrier liner200344
US 6,531,192 B2Chemical vapor deposition process for depositing titanium nitride films from an organo-metallic compound200318
US 6,534,398 B2Method of forming metal layer(s) and/or antireflective coating layer(s) on an integrated circuit20032
US 6,627,547 B2Hot metallization process20034
US 6,656,831 B1Plasma-enhanced chemical vapor deposition of a metal nitride layer200323
US 6,756,302 B1Low temperature metallization process200418

Non-Patent Literature (4)

  • Likeda Takaaki; Method of Manufacturing Semiconductor Device; Jan. 31, 2002; Patent Abstracts of Japan; Publication No. 2002-033322; Japanese Intellectual Property Office, Japan.
  • Office Action, Korean Patent Application No. 10-2003-010278; dated Aug. 19, 2005.
  • Partial English translation of foreign patent document believed to be Korean Patent Publication No. 10-1999-6153.
  • Ted Guo and Wei Ti Lee; Method for Plasma-Enhanced Chemical Vapor Deposition of Metal Nitride Layer; Aug. 20, 2001; Korean Patent Abstracts; Publication No. 1020010078086 A; Korean Intellectual Property Office, Republic of Korea.