Shallow low energy ion implantation into pad oxide for improving threshold voltage stability
Abstract
A method is described to fabricate a MOSFET device with increased threshold voltage stability. After the pad oxide and pad nitride are deposited on the silicon substrate and shallow trenches are patterned and the pad nitride removed. As + or P + species are then implanted using low energy ions of approximately 5 keV into the pad oxide. Conventional As + or P + implant follows the shallow implant to form the n-wells. With this procedure of forming a sacrificial shallow implantation oxide layer, surface dopant concentration variation at pad oxide:silicon substrate interface is minimized; and threshold voltage stability variation of the device is significantly decreased.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 1.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of forming a semiconductor device, the steps comprising: forming a silicon dioxide layer on a semiconductor substrate; forming a silicon nitride layer on said silicon dioxide layer; forming isolation trench regions in said semiconductor substrate; removing said silicon nitride layer; first blanket implantation of dopant through said silicon dioxide to form sacrificial blanket implanted silicon dioxide layer; second blanket implantation of dopant through said sacrificial blanket implanted silicon dioxide layer to form wells; and removing said sacrificial blanket implanted silicon dioxi
- Claim 2Depends on #1
The method of forming a semiconductor device according to claim 1 , wherein said silicon dioxide layer thickness is approximately about 25 Å-120 Å.
- Claim 3Independent Claim
The method of formi
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗