Method to solve via poisoning for porous low-k dielectric
Abstract
A method of forming a via in a low-k dielectric material and without the attendant via poisoning problem, or a dual damascene structure formed in the same dielectric and without the same problem are disclosed. The vertical walls of the via opening are first lined with a low-k protection layer and then covered with a barrier layer in order to prevent outgassing from the low-k dielectric material when copper is deposited into the via opening. In the case of a dual damascene structure, it is sufficient that the hole opening underlying the trench opening is first lined with the low-k protection layer. The resulting via or dual damascene structure is free of poisoned metal and, therefore, more reliable.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 8.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A damascene structure with a protection layer for low-k materials comprising: a substrate having a damascene structure with an upper trench opening and a lower hole opening formed in a low-k dielectric layer; a low-k protection layer on the vertical walls of said lower hole opening; a barrier layer over said low-k protection layer on said vertical walls of said lower hole opening, and on the vertical walls of said trench opening; and a metal layer deposited in said dual damascene structure; wherein said low-k dielectric layer includes at least one of black diamond, CVD SiC, SiLK, and a polymer
- Claim 2Depends on #1
The damascene structure according to claim 1 , including a passivation layer disposed below said low-k dielectric layer with said lower hole opening, said passivation layer havin