Resin molded product and fuel tank
Abstract
A fuel tank produced in such a manner that an upper shell and a lower shell melt-molded as two split molded parts from a PPS resin composition are welded to each other at a welding portion. The PPS resin composition contains (a) 60% by weight to 95% by weight of a PPS resin, and (b) 5% by weight to 40% by weight of an olefin resin. The (a) PPS resin contains (a-1) a PPS resin having an MFR of 90 g/10 min to 350 g/10 min and an amount of extracts by chloroform of 2.2% by weight to 4.5% by weight. The (b) olefin resin contains (b-1) a specific olefin copolymer, and (b-2) an ethylene-α-olefin copolymer. The MFR of the PPS resin composition is 15 g/10 min to 50 g/10 min.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 34 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A resin molded product by melt molding of a polyphenylene sulfide resin composition, said polyphenylene sulfide resin composition comprising: (a) 60% by weight to 95% by weight of polyphenylene sulfide resin, and (b) 5% by weight to 40% by weight of an olefin resin; said (a) polyphenylene sulfide resin comprising: (a-1) 100 parts by weight of a polyphenylene sulfide resin that is not cross-linked by thermal oxidation and having a melt flow rate (315.5° C., 5000 g load) of 90 g/10 min to 350 g/10 min measured according to ASTM-D1238, and an amount of extracts by chloroform of 2.2% by weight to
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (34)
Non-Patent Literature (1)
- Derwent Abstract of JP 2001/0160011 A to Nishimura et al., 'Polyphenylene Sulfide Resin Composition'; Jun. 13, 2000.