Method of wet cleaning a surface, especially of a material of the silicon-germanium type
Abstract
Method of wet cleaning a surface of at least one material chosen from silicon, silicon-germanium alloys, A(III)/B(V)-type semiconductors and epitaxially grown crystalline materials, such as germanium, in which method the following successive steps are carried out: a) the surface is brought into contact with an HF solution; b) the surface is rinsed with acidified, deionized water, then a powerful oxidizing agent is added to the deionized water and the rinsing is continued; c) optionally, step a) is repeated, once or twice, while optionally reducing the contacting time; d) step b) is optionally repeated, once or twice; and e) the surface is dried. Process for fabricating an electronic, optical or optoelectronic device, such as a CMOS or MOSFET device, comprising at least one wet cleaning step using the said cleaning method.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 18.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of wet cleaning a surface in which the following successive steps are carried out: a o ) the surface is brought into contact with an H 2 SO 4 solution to which 0.5 vol % or less of H 2 O 2 has been added, for a time of about 5 minutes; a) the surface is brought into contact with an HF/HCL solution, having respective concentrations of 0.2 vol % and 1 vol %, in deionized water, for a time of about 4 minutes; b) the surface is rinsed with a 0.01 wt % HCL solution in deionized water for a time of about 3 minutes; c) the surface is rinsed with a 0.01 vol % HCL solution in deionized water
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 18 total)
References Cited — Backward Prior Art (10)
Non-Patent Literature (5)
- Hartmann et al. "Gas-source molecular beam epitaxy of SiGe virtual substrates: II. Strain relaxation and surface morphology" Semicond. Sci. Technol. 15:370-377 (2000).
- Sawano et al. "Surface Planarization of Strain-Relaxed SiGe Buffer Layers by CMP and Post Cleaning" Journal of The Electrochemical Society 150(7):G376-G379 (2003).
- Sawano et al. "Surface smoothing of SiGe strain-relaxed buffer layers by chemical mechanical polishing" Materials Science and Engineering B89:406-409 (2002).
- Tardif et al. Diluted Dynamic Clean : "DDC" Proceedings of the 3<SUP>rd </SUP>International Symposium on Ultra clean Processing of Silicon Surfaces, Antwerp. Belgium pp. 175-178 (1996).
- Tardif, et al. "New Aspects of the Diluted Dynamic Clean Process" Solid State Phenomena vol. 65-66:19-22 (1999).