Low stress STI films and methods

4Forward Citations (#26550796 Global)
0.2/yrCitation Velocity (#32365565 Global)
1.19Citation PageRank (#32646126 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention generally relates to low compressive stress doped silicate glass films for STI applications. By way of non-limited example, the stress-lowering dopant may be a fluorine dopant, a germanium dopant, or a phosphorous dopant. The low compressive stress STI films will generally exhibit a compressive stress of less than 180 MPa, and preferably less than about 170 MPa. In certain embodiment, the STI films of the invention will exhibit a compressive stress less than about 100 MPa. Further, in certain embodiments, the low compressive stress STI films of the invention will comprise between about 0.1 and 25 atomic % of the stress-lowering dopant.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of depositing a low compressive stress, shallow trench isolation (STI) film with good gap fill characteristics on a substrate, said method comprising: (a) positioning a substrate in a deposition chamber, wherein said substrate comprises at least one isolation trench between adjacent raised surfaces formed by anisotropic etching; (b) providing a gas mixture to the deposition chamber in one or more steps, wherein the gas mixture comprises a silicon source gas, a stress-lowering dopant source gas, at least one fluent source gas, and an oxidizer; (c) reacting the gas mixture in the presen

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗