A process for manufacturing a cellulosic paper product is provided. The process comprises forming an aqueous suspension of papermaking fibers; depositing the aqueous suspension onto a sheet-forming fabric to form a wet web; dewatering the wet web to form a partially dewatered web; topically applying a glycol compound selected from the group consisting of polyethylene glycol, triethylene glycol, glycerol and mixtures thereof to the partially dewatered web; and drying said wet web. The present invention also provides for cellulosic paper products exhibiting a reduced malodor upon wetting.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 35 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for manufacturing a cellulosic paper product, the process comprising: forming an aqueous suspension of papermaking fibers; depositing said aqueous suspension of papermaking fibers onto a sheet-forming fabric to form a wet web; dewatering said wet web to form a partially dewatered web; topically applying a glycol compound selected from the group consisting of polyethylene glycol, triethylene glycol, glycerol and mixtures thereof to said partially dewatered web, said partially dewatered web having a fiber consistency of about 80% or less; and drying said partially dewatered web by pass

  2. Claim 2Depends on #1

    A process as set forth in claim 1 wherein said glycol compound is polyethylene glycol having a molecular weight of from about 400 to about 800.

  3. Claim 3Independent Claim

    A process as set f

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (35)

PatentTitleYearCitations
US 3,303,576 AApparatus for drying porous paper1967132
US 3,840,395 AStabilized glycol plasticized cellulosic sheets19749
US 4,002,486 AGlyoxal composition197710
US 4,863,987 ADeodorizing coating formulations and deodorizing sheets making use of same198912
US 4,994,146 ACreping adhesive utilizing polymer-polymer complex formation199161
US 5,048,589 ANon-creped hand or wiper towel1991280
US 5,122,407 AOdor-removing cover for absorbent pads and method of making same1992121
US 5,300,192 AWet laid fiber sheet manufacturing with reactivatable binders for binding particles to fibers1994114
US 5,308,896 AParticle binders for high bulk fibers1994115
US 5,352,480 AMethod for binding particles to fibers using reactivatable binders199468
WO 9,608,601 A1Tissue paper treating agent, process for producing tissue paper by using said treating agent and its use—28
US 5,575,891 ASoft tissue paper containing an oil and a polyhydroxy compound199651
WO 9,706,306 A1Lotioned tissue paper containing an emollient and a polyol polyester—7
WO 9,706,307 A1Lotioned tissue paper containing a liquid polyol polyester emollient and an immobilizing agent—6
US 5,624,532 AMethod for enhancing the bulk softness of tissue paper and product therefrom199752
US 5,624,676 ALotioned tissue paper containing an emollient and a polyol polyester immobilizing agent199762
US 5,705,164 ALotioned tissue paper containing a liquid polyol polyester emollient and an immobilizing agent199855
US 5,981,044 AMulti-layered tissue paper web comprising biodegradable chemical softening compositions and binder materials and process for making the same199977
US 5,998,032 AMethod and compositions for enhancing blood absorbence by superabsorbent materials199970
US 6,033,523 AMethod of making soft bulky single ply tissue200081
US 6,068,731 ASoft, bulky single-ply tissue having low sidedness and method for its manufacture200035
US 6,120,644 ATissue containing cationic amidoamine compounds200012
US 6,126,784 AProcess for applying chemical papermaking additives to web substrate200080
US 6,143,131 ASoft bulky single-ply tissue having low sidedness and method for its manufacture200027
US 6,149,767 AMethod for making soft tissue200096
US 6,156,157 AMethod for making soft tissue with improved bulk softness and surface softness200011
US 6,162,329 ASoft tissue paper having a softening composition containing an electrolyte deposited thereon200081
US 6,187,141 B1Water-disintegratable fibrous sheet having layered structure and wiping sheet comprising the same200135
US 6,190,735 B1Process for treating a fibrous material and article thereof200136

Non-Patent Literature (5)

  • Cullis, C.F., et al., "Combustion of Cigarette Paper Under Conditions Similar to Those During Smoking", Cellulose & Its Derivatives, 1985, Chapter 35, Kennedy et al., eds., Ellis Horwood Ltd.
  • International Search Report from PCT/US 02/39570 dated Sep. 29, 2003.
  • International Search Report from PCT/US 2004/000861 dated Jun. 29, 2004.
  • K.Wiik, et al., "Studies on Odour Reduction in TCF Bleached Packaging Paper", Journal of Pulp and Paper Science, Sep. 1998, vol. 24, No. 9.
  • LeVan, S.L., "Chemistry of Fire Retardancy", The Chemistry of Solid Wood, 1984, Chapter 14, R. Rowell, editor, Advances in Chemistry Series 207 American Chemical Society.