Patents
US 7,228,722 B2#13984517 Most CitedExpiredUnited States (USPTO)Utility

Method of forming sputtering articles by multidirectional deformation

8Forward Citations (#13984517 Global)
0.4/yrCitation Velocity (#19375169 Global)
1.38Citation PageRank (#26075654 Global)
24Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of producing a valve metal mill form having dimensions sufficient to be divided to form a plurality of sputter targets is described. The method includes multidirectional deformation of an ingot to form a mill form having a preferred average grain size of about 100 microns or less and/or a texture substantially void of textural bands.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of producing a multidirectionally deformed valve metal having dimensions sufficient to be divided to form a plurality of sputter targets, comprising: a first deforming of an ingot to form a preform slab having a first dimension, a second dimension normal to said first dimension, and a third dimension normal to said second dimension that is less than both said first and said second dimensions; and a second deforming of said preform slab by increasing said third dimension and decreasing said second dimension such that said second dimension is made to be less than said third dimension to

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising partitioning said intermediate slab to form a plurality of rolling slabs.

  3. Claim 3Depends on #1

    The method of claim 1

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 4,721,537 AMethod of producing a fine grain aluminum alloy using three axes deformation198845
US 4,844,746 AMethod of producing a tantalum stock material of high ductility198951
US 5,390,518 AMethod for shining metal sheet surfaces and method for cold-rolling metallic materials199513
US 5,615,465 AProcess for manufacturing metal parts by free forging and drop forging in a press199719
US 5,647,923 AMethod for producing refractory metal foil19975
US 6,193,821 B1Fine grain tantalum sputtering target and fabrication process200162
US 6,238,494 B1Polycrystalline, metallic sputtering target200185
US 6,312,642 B1Method for controlling the oxygen content in valve metal materials200156
US 6,331,233 B1Tantalum sputtering target with fine grains and uniform texture and method of manufacture2001103
US 6,348,139 B1Tantalum-comprising articles200276
US 6,348,113 B1High purity tantalum, products containing the same, and methods of making the same2002117
US 2002026965 A1High purity tantalum, products containing the same, and methods of making the same—18
US 2002063056 A1Methods of forming metal articles—26
US 2002072475 A1High purity niobium and products containing the same, and methods of making the same—27
US 2002112789 A1Refractory metal plates with uniform texture and methods of making the same—50
US 2002125128 A1Tantalum sputtering target with fine grains and uniform texture and method of manufacture—18
US 2002153071 A1Methods of fabricating metallic materials—28
US 2002153248 A1Methods of forming metal articles—8
US 2003019746 A1Hollow cathode target and methods of making same—22
US 2003037847 A1High purity tantalum, products containing the same, and methods of making the same—17
US 2003089429 A1Textured-grain-powder metallurgy tantalum sputter target—17
US 6,569,270 B2Process for producing a metal article200338

Non-Patent Literature (2)

  • International Search Report for PCT/US2004/017972.
  • Written Opinion for PCT/US2004/017972.