Patents
US 7,226,885 B2#24839691 Most CitedExpiredUnited States (USPTO)Utility

Method for producing gas diffusion electrodes

4Forward Citations (#24839691 Global)
0.2/yrCitation Velocity (#32245179 Global)
1.37Citation PageRank (#26315071 Global)
21Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

With the help of a method for production of a gaseous diffusion electrode from a silver catalyst on PTFE-substrate, it is endeavored to achieve results which can be reproduced, by avoiding the disadvantages of the state-of-the-art technology, whereby this is achieved in that the porous system of the silver catalyst is filled with a wetted fluid; a dimension-stable solid body with a grain size above that of the silver catalyst is mixed below the silver catalyst; the thus compression-stable mass is shaped into a homogenous catalyst band in a calender; and in a second calender step, an electrically conductive conductor material is imprinted into the catalyst band.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 4.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Method for producing a gaseous diffusion electrode from a silver catalyst on a PTFE-substrate, comprising the steps of: filling a porous system of the silver catalyst with a wetting fluid; mixing a dimension-stable solid body with a grain size above that of the silver catalyst with the silver catalyst to produce a compression-stable mass; shaping the thus obtained compression-stable mass into a homogeneous catalyst band in a calender, and in a second calender step, imprinting an electrically conducting material into the catalyst band.

  2. Claim 2Depends on #1

    Method as per claim 1 , comprising using as wetting fluid 5% isopropanol and as solid substance 30% ammonium carbonate or ammonium-hydrogen-carbonate and driving both these filling substances out after producing the electrodes by means of an annealing step at preferably 110° C.

  3. Claim 3Independent Claim

    Method as per c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗