Patents
US 7,223,497 B2#56885074 Most CitedExpiredUnited States (USPTO)Utility

Hydrogen storage alloy, process for producing hydrogen storage alloy, hydrogen storage alloy electrode, process for producing hydrogen storage alloy electrode, and battery

1Forward Citations (#56885074 Global)
0.1/yrCitation Velocity (#54666226 Global)
0.80Citation PageRank (#56885074 Global)
29Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Hydrogen storage alloy has: (1) a main composition expressed by the formula of Mm-(Ni—Al—Co—Mn—Mo); (2) a ratio of the number of atoms expressed by the formula of (Ni—Al—Co—Mn—Mo) is 5.7<(Ni+Al+Co+Mn+Mo)≦8, and 3.5≦Ni, when Mm is set at 1 in a ratio of the number of atoms; and (3) an internal structure having hydrogen storage alloy phase expressed by the general formula of AB 5 , and a second phase existing in the hydrogen storage alloy phase.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Hydrogen storage alloy comprising: (1) a main composition expressed by the formula of Mm—(Ni—Al—Co—Mn—Mo); (2) a ratio of the number of atoms expressed by the formula of (Ni—Al—Co—Mn—Mo) is exhibited as 6.5<(Ni+Al+Co+Mn+Mo)≦8, and 3.5≦Ni, when Mm is set at 1 in a ratio of the number of atoms; and (3) an internal structure having a hydrogen storage alloy phase expressed by the general formula of AB 5 , and a second phase existing in said hydrogen storage alloy phase.

  2. Claim 2Depends on #1

    Hydrogen storage alloy according to claim 1 , wherein said second phase having a crystal structure exhibiting a μ-NiMoCo type or a Co 7 Mo 6 type.

  3. Claim 3Depends on #1

    Hydrogen storage alloy according to claim 1 , wherein said whole composition is expressed by the formula of MmNi (3.55+i) Al (0.3+j) Co (0.75+k) Mn (0.4+1) Mo (m) , and 1.5<( i+j+k+l+m )≦3.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
JP S60250558 AEnclosed type alkaline storage battery—27
JP S63291363 AHydrogen absorption alloy—11
JP H0346770 AElectrochemical battery and electro- chemical active substance and its manufacture—5
JP H04168240 AHydrogen storage alloy—4
JP H04328256 AHydrogen storage alloy for nickel-hydrogen battery and manufacture thereof—9
US 5,185,221 AMetal hydride electrode and electrochemical cell199322
EP 0,557,656 A1Hydrogen storage alloy electrode—8
EP 0,557,522 A1Hydrogen-storing electrode, nickel electrode, and nickel-hydrogen battery—22
US 5,306,583 AHydridable material for the negative electrode of a nickel-hydride storage cell199411
JP H06150919 AMetallic oxide-hydrogen secondary battery—6
JP H06256873 AHydrogen storage alloy and electrode using the alloy—5
JP H06306411 AProduction of hydrogen storage alloy powder—5
JP H0750163 AHydrogen storage alloy electrode and manufacture thereof—3
JP H07157813 AActivation treatment for hydrogen storage alloy—5
JP H07230807 AManufacture of metal oxide-hydrogen secondary battery—4
JP H07258703 APowdery hydrogen occluding alloy and its production—7
JP H07268519 AHydrogen storage alloy for battery, its production and nickel hydrogen battery—13
JP H07278708 AHydrogen storage alloy and electrode of it—8
JP H07286225 AHydrogen storage alloy and nickel-hydrogen storage battery using the same—16
US 5,529,857 AHydrogen-absorbing alloy electrode and process for producing the same199620
JP H08250115 AAlkaline secondary battery—3
JP H08315815 AManufacture of hydrogen storage alloy for alkaline storage battery—3
JP H08315813 AHydrogen storage alloy electrode for alkaline storage battery—3
EP 0,751,229 A1Age-precipitating rare earth metal-nickel alloy, its manufacture, and negative electrode for nickel-hydrogen secondary cell—14
JP H0931573 AHydrogen storage alloy and its production—7
EP 0,765,947 A1Rare earth metal-nickel hydrogen-occlusion alloy, process for producing the same, and negative electrode of nickel-hydrogen secondary battery—8
JP H0997607 AHydrogen storage alloy for battery, manufacture thereof, and nickel hydrogen secondary battery—4
US 5,753,386 AHydrogen-absorbing alloy for battery and secondary nickel-metal hydride battery199819
US 6,053,995 AMethod of producing an age precipitation-containing rare earth metal-nickel alloy200011

Non-Patent Literature (5)

  • Cunmao et al., "Second Phase and Electrode Characteristics of Rare-Earth-Based AB5+x Alloys", Journal of Alloys and Compounds, 231, 1995, pp. 546-549, no month.
  • Fukumoto et al., "Effect of alloy composition on enthalpy and entropy changes of hydride formation for stoichiometric and nonstoichiometric hydrogen storage alloys", J. of Alloys and Compounds, 240, pp. 76-78, no month 1996.
  • Fukumoto et al., "Effect of the Stoichiometric Ratio on Electrochemical Properties of Hydrogen Storage Alloys for Nickel-Metal Hydride-Batteries", Electrochimica Acta, vol. 40, No. 7, pp. 845-848, 1995, no month.
  • IPDL JPO Machine Translation for JP 07-268519 A (publication date of Oct. 1995).
  • IPDL JPO Machine Translation for JP 09-031573 A (publication date of Apr. 1997).