Patents
US 7,218,007 B2#8551213 Most CitedExpiredUnited States (USPTO)Utility

Underfill material to reduce ball limiting metallurgy delamination and cracking potential in semiconductor devices

12Forward Citations (#8551213 Global)
0.6/yrCitation Velocity (#12551815 Global)
2.04Citation PageRank (#14037589 Global)
16Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An electronic structure includes an electronic device coupled to a substrate by conductive bumps and ball limiting metallurgy (BLM). Underfill material having filler particles is disposed in a space between the electronic device and the substrate. A weight percentage of the filler particles is at least about 60%. A particle size of at least 90 wt % of the filler particles is less than about 2 μm and/or the filler particles are coated by an organic coupling agent. Once the underfill material is fully cured, its coefficient of thermal expansion is no more than 30 PPM/° C., and its glass transition temperature is at least 100° C., and its adhesion to a passivation layer of the electronic device, to the substrate and to the electronic device at its edges is such that the electronic structure passes standardized reliability tests without delamination of the ball limiting metallurgy.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An underfill material for use with a semiconductor die device coupled to a substrate by conductive bumps and ball limiting metallurgy, said underfill material comprising: filler particles, wherein a weight percentage of said filler particles in said underfill material is at least about 60%, wherein a particle size of at least 90wt % of said filler particles is less than about 2 μm or said filler particles are coated by an organic coupling agent, wherein a coefficient of thermal expansion of said underfill material, once fully cured, is no more than 30PPM/° C., wherein if said underfill materia

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (16)

PatentTitleYearCitations
US 3,613,613 AClosure member coating composition comprising an organosol-solution of polyvinyl chloride, acrylonitrile-butadiene copolymer, and phenolic resole resin19716
US 5,340,781 ASpherical corundum particles, process for preparation thereof and rubber or plastic composition having high thermal conductivity and having spherical corundum paticles incorporated therein199444
US 5,567,792 ASpherical curing agent for epoxy resin, curing agent masterbatch for epoxy resin and their preparation19968
US 5,629,566 AFlip-chip semiconductor devices having two encapsulants1997152
US 5,677,045 ALaminate and multilayer printed circuit board199774
US 5,855,821 AMaterials for semiconductor device assemblies1999116
US 5,930,597 AReworkable polymer chip encapsulant199937
US 5,998,861 ASemiconductor device having ball grid array199969
US 6,121,689 ASemiconductor flip-chip package and method for the fabrication thereof2000234
US 6,132,646 APolmerizable fluxing agents and fluxing adhesive compositions therefrom200060
US 6,297,564 B1Electronic devices employing adhesive interconnections including plated particles200135
US 6,326,241 B1Solderless flip-chip assembly and method and material for same200138
US 6,376,160 B1Protective epoxy overcoat for photographic elements20027
US 6,774,493 B2Semiconductor flip-chip package and method for the fabrication thereof200470
US 6,784,555 B2Die attach adhesives for semiconductor applications utilizing a polymeric base material with inorganic insulator particles of various sizes200434
US 6,943,058 B2No-flow underfill process and material therefor20059