Methods to form electronic devices and methods to form a material over a semiconductive substrate
Abstract
A first electrode and a doped oxide layer laterally proximate thereof are provided over a substrate. A silicon nitride layer is formed over both the doped oxide layer and the first electrode to a thickness of no greater than 80 Angstroms over at least the first electrode by low pressure chemical vapor deposition using feed gases comprising a silicon hydride, H 2 and ammonia. The substrate with silicon nitride layer is exposed to oxidizing conditions comprising at least 700° C. to form a silicon dioxide layer over the silicon nitride layer, with the thickness of silicon nitride over the doped oxide layer being sufficient to shield oxidizable substrate material beneath the doped oxide layer from oxidizing during the exposing. A second electrode is formed over the silicon dioxide layer and the first electrode. In one implementation, the chemical vapor depositing comprises feed gases of a silicon hydride and ammonia, with the depositing comprising increasing internal reactor temperature from below 500° C. to a maximum deposition temperature above 600° C. and starting feed of the silicon hydride into the reactor at a temperature less than or equal to 600° C. In one implementation the de
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 38 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming an electronic device comprising: providing a first electrode and a doped oxide layer laterally proximate thereof over a substrate; forming a silicon nitride layer over both the doped oxide layer and the first electrode to a thickness of no greater than 80 Angstroms over at least the first electrode by low pressure chemical vapor deposition using feed gases comprising a silicon hydride, H 2 and ammonia, initial feed of the silicon hydride to the reactor commencing at a temperature of no greater than 600° C.; exposing the substrate with silicon nitride layer to oxidizing con
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (38)
Non-Patent Literature (3)
- DeBoer, S.J., et al., "Thin Nitride Films: Pushing The Limits Using Rapid Thermal Processing", Mat. Res. Soc. Symp. Proc., Materials Research Society, vol. 429 (1996).
- Jeon, Yongjoo, et al., "Effect of Barrier Layer on the Electrical and Reliability Characteristics of High-k Gate Dielectric Films", IEEE, pp. 29.6.1 (1998).
- Thakur, R.P.S., et al., "Rapid Thermal Processing-Manufacturing Perspective", Mat. Res. Soc. Symp. Proc., Materials Research Society, vol. 387 (1995).