Abstract

An improved steel railroad rail, and methods for producing same, having a carbon content in a range from 0.7 to 0.95 wt % and titanium in the range of 0.005 to 0.105 wt % is provided that has increased wear resistance and increased fracture toughness over conventional steel rail. The rail is characterized as having a pearlitic phase of an eutectoid nature. The average ultimate tensile strength is in a range from 178,000 to 207,000 psi, with a minimum of 174,000 psi. The average yield strength is in a range from 122,000 to 141,000 psi, with the minimum of 120,000 psi. The average percent elongation is in a range from 10.3 to 12.5, with a minimum of 10.00. The Brinell hardness on the surface at any position of the head top and upper gage corners of the rail is in a range from 370 to 420 BHN. The hardness 19 mm below the top surface is in a range from 360 to 405 BHN and 19 mm below the surface at the upper gage corners is in a range from 360 to 410 BHN. The characteristics of the steel rail produced in accordance with the present invention is a substantial improvement as compared with rail used today. The production of a fully pearlitic steel rail having a carbon content from 0.7 to 0

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 15.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a fully pearlitic steel rail of high toughness and high wear resistance consisting essentially of: forging a steel billet comprising the elements in a range from 0.7 to 0.95 wt % of C, 0.005 to 0.105 wt % of Ti, 0.26 to 0.80 by wt % of Si, 0.8 to 1.2 wt % of Mn, less than or equal to 0.35 wt % of Cr, the balance of iron and residual elements; hot rolling the billet such that the rolling finishing temperature is about 1000.degree.C, thereby forming a rail; and heat treating by cooling the rail at a cooling rate in a range from 3.3.degree.C./sec to 4.3.degree.C./sec. b

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the steel comprises a maximum of each of the elements 0.45 wt % of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗