Method to produce thin film resistor using dry etch

4Forward Citations (#23205755 Global)
0.2/yrCitation Velocity (#32088960 Global)
1.80Citation PageRank (#17239155 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of fabricating a thin film resistor ( 100 ). The resistor material ( 104 ), e.g., NiCr, is deposited. A hard mask material ( 106 ), e.g., TiW, may be deposited over the resistor material ( 104 ). The resistor material ( 104 ) and hard mask material ( 106 ) are patterned and sputter etched to form the resistor body. For example, a sputter etch chemistry comprising BCl 3 , Cl 2 , and Ar may be used to etch the resistor material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating an integrated circuit, comprising the steps of: depositing a layer of resistor material; forming a pattern over said layer of resistor material; and sputtering etching said layer of resistor material to form a thin film resistor body, wherein said sputter etching strip comprises the steps of: flowing BCl 3 at a flow rate of about 15 sccm; flowing Cl 2 at a flow rate of about 55 sccm; and flowing Ar at a flow rate of about 15 sccm.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said layer of resistor material comprises NiCr.

  3. Claim 3Depends on #1

    The method of claim 1 , further comprising the steps of: depositing a hard mask layer over said layer of resistor material; and after forming said pattern, sputter etching said hard mask material prior to sputter etching said layer of resistor material.