Production of polypropylene fine monofilaments, polypropylene fine monofilaments and use thereof
Abstract
In a process for producing fine monofilaments having improved abrasion resistance from a polypropylene having a melt flow index (MFI) 230° C./2.16 kg of 2–16 g/10 min at a linear density of 5–20 dtex (0.027 mm–0.053 mm), a compound consisting of 80 to 99.9% by weight of chips and 20 to 0.1% by weight of an additive is added to the extruder, the melt is spun at a speed of at least 1200 m/min, the fibre is cooled in an air bath at room temperature, supplementarily stretched at a temperature of 110–150° C. to a linear density of 5–20 dtex and wound up. The monofilaments comprising a polypropylene having a melt flow index (MFI) 230° C./2.16 kg of 2–16 g/10 min, having improved abrasion resistance, and a linear density of 5–20 dtex (0.027 mm–0.053 mm) and an abrasion resistance score ≦2. The monofilaments have a tenacity of at least 48 cN/tex and an elongation at break of less than 45% for a mechanical constant (constante méchanique) of at least 295 cN/tex and a specific work to break value of more than 61.5 cN·cm/dtex. The fine monofilaments according to the invention are useful for producing woven screen fabrics for filtration and screen printing without abrasion deposits.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 1.
Claims (3 — 3 Independent, 0 Dependent)
- Claim 1Independent Claim
Monofilaments, comprising a polypropylene having a melt flow index (MEI) 230° C./2.16 kg of 2–16 g/10 mm and having improved abrasion resistance, having a linear density of 5–20 dtex (0.027 mm–0.053 mm), and having a tenacity of at least 47 cN/tex and an elongation at break of less than 45%.
- Claim 2Independent Claim
Monofilaments, comprising a polypropylene having a melt flow index (MFI) 230° C./2.16 kg of 2–16 g/10 min and having improved abrasion resistance, having a linear density of 5–20 dtex (0.027 mm–0.053 mm), and having a mechanical constant (constante méchanique) of at least 285 cN/tex.
- Claim 3Independent Claim
Monofilaments, comprising a polypropylene having a melt flow index (MEI) 230° C./ 2.16 kg of 2–16 g/10 min and having improved abrasion resistance, having a linear density of 5–20 dtex (0.027 mm–0.053 mm), and having a specific work to break value of more than 61.5 cNcm/dtex.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2007264500 A1 | Polypropylene-Based Monofilaments With Improved Properties | — | 1 |