US 7,213,329 B2#2855072 Most CitedExpiredUnited States (USPTO)Utility

Method of forming a solder ball on a board and the board

26Forward Citations (#2855072 Global)
1.4/yrCitation Velocity (#4107942 Global)
4.01Citation PageRank (#4752339 Global)
16Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In the method, a conductive pad of the board is etched to a depth that is greater than 50% and less than 100% of a thickness of the conductive pad. Subsequently, a solder ball may be formed on the etched conductive pad. For example, the conductive pad may be copper.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 26.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a solder ball on a board, comprising: etching a conductive pad of the board, a depth of the etching being greater than 60% and less than 90% of a thickness of the conductive pad; forming a solder ball on the etched conductive pad; forming a photo solder resist layer over the board such that at least a portion of the conductive pad is exposed; and wherein the etching step etches part of the conductive pad disposed under the photo solder resist layer.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the solder ball is a lead free solder ball.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the solder ball include tin, silver and copper.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗