US 7,211,499 B2#65600571 Most CitedActiveUnited States (USPTO)Utility

Methods of forming silicon dioxide layers, and methods of forming trench isolation regions

0Forward Citations (#65600571 Global)
0.0/yrCitation Velocity (#65600571 Global)
0.56Citation PageRank (#65600571 Global)
47Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of forming a silicon dioxide layer includes forming a high density plasma proximate a substrate, the plasma comprising silicon dioxide precursors; forming silicon dioxide from the precursors, the silicon dioxide being deposited over the substrate at a deposition rate; and while depositing, etching the deposited silicon dioxide with the plasma at an etch rate; a ratio of the deposition rate to the etch rate being at least about 4:1. Another method includes forming a high density plasma proximate a substrate; flowing gases into the plasma, at least some of the gases forming silicon dioxide; depositing the silicon dioxide formed from the gases over the substrate; and while depositing the silicon dioxide, maintaining a temperature of the substrate at greater than or equal to about 500° C. As an alternative, the method may include not cooling the substrate with a coolant gas while depositing the silicon dioxide.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 47 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a silicon dioxide layer, comprising: generating a high density plasma proximate a semiconductive substrate in a reaction chamber; flowing gases into the plasma, at least some of the gases forming silicon dioxide; depositing the silicon dioxide formed from the gases over the substrate; and while depositing the silicon dioxide, maintaining a temperature of the substrate at greater than 700° C. to about 1000° C.

  2. Claim 2Depends on #1

    The method of claim 1 further comprising: forming openings in the substrate; and depositing the silicon dioxide within the openings.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the gases comprise SiH 4 and oxygen.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (47)

PatentTitleYearCitations
US 4,839,306 AMethod of manufacturing a trench filled with an insulating material in a semiconductor substrate198966
US 5,270,264 AProcess for filling submicron spaces with dielectric1993148
JP H0776777 AMethod and device for forming silicon oxide film—6
US 5,447,884 AShallow trench isolation with thin nitride liner1995263
JP H088232 APlasma treatment method—21
US 5,494,854 AEnhancement in throughput and planarity during CMP using a dielectric stack containing HDP-SiO2 films1996141
US 5,531,834 APlasma film forming method and apparatus and plasma processing apparatus1996152
US 5,614,055 AHigh density plasma CVD and etching reactor1997343
WO 9,724,761 A1Methods and apparatus for filling trenches in a semiconductor wafer—12
US 5,660,895 ALow-temperature plasma-enhanced chemical vapor deposition of silicon oxide films and fluorinated silicon oxide films using disilane as a silicon precursor199790
US 5,679,606 Amethod of forming inter-metal-dielectric structure1997132
US 5,726,097 AMethod of forming multilevel interconnections using high density plasma metal clean199847
US 5,726,090 AGap-filling of O3 -TEOS for shallow trench isolation199869
US 5,731,241 ASelf-aligned sacrificial oxide for shallow trench isolation199885
EP 0,843,348 A2Method and apparatus for processing a semiconductor substrate—41
US 5,763,315 AShallow trench isolation with oxide-nitride/oxynitride liner1998198
US 5,872,058 AHigh aspect ratio gapfill process by using HDP1999185
JP H11154673 AManufacture of semiconductor device—12
US 5,966,616 AMethod of manufacturing a semiconductor device having "shallow trench isolation"199927
US 5,968,610 AMulti-step high density plasma chemical vapor deposition process1999114
US 5,976,993 AMethod for reducing the intrinsic stress of high density plasma films199944
US 6,013,584 AMethods and apparatus for forming HDP-CVD PSG film used for advanced pre-metal dielectric layer applications200096
US 6,015,759 ASurface modification of semiconductors using electromagnetic radiation200068
US 6,030,881 AHigh throughput chemical vapor deposition process capable of filling high aspect ratio structures2000301
US 6,077,786 AMethods and apparatus for filling high aspect ratio structures with silicate glass200036
US 6,103,601 AMethod and apparatus for improving film stability of halogen-doped silicon oxide films200064
US 6,110,544 AProtective coating by high rate arc plasma deposition200090
US 6,114,216 AMethods for shallow trench isolation200096
US 6,136,685 AHigh deposition rate recipe for low dielectric constant films200077
US 6,140,208 AShallow trench isolation (STI) with bilayer of oxide-nitride for VLSI applications200071

Non-Patent Literature (3)

  • Gross, M., "Silicon Dioxide Trench Filing Process in a Radio-Frequency Hollow Cathode Reacto", J. Vac. Sci. Tech., B11(2), Mar./Apr. 1993, No. 2, pp. 242-248.
  • Jung et al., "Enhancing uniformity of borderless VIA resistance by HDP oxide technology", ST-P06 07-803-5727-2/99, pp. 452-455.
  • Lee et al., "A Low Redeposition Rate High Density Plasma CVD Process for High Aspect Ratio 175 nm Technology and Beyond", IITC 99, pp. 152-154 0-7803-5174-6/99, IEEE.