Permanent adherence of the back end of a wafer to an electrical component or sub-assembly
Abstract
A plurality of successive layers are firmly adhered to one another and to a wafer surface and an electrical component or sub-assembly even when the wafer surface is not even and the layers are bent. The wafer surface is initially cleaned by an ion bombardment of an inert gas (e.g. argon) on the wafer surface in an RF discharge at a relatively high gas pressure. The wafer surface is then provided with a microscopic roughness by applying a low power so that the inert gas (e.g. argon) ions do not have sufficient energy to etch the surface. A layer of chromium is then sputter deposited on the wafer surface as by a DC magnetron with an intrinsic tensile stress and low gas entrapment by passing a minimal amount of the inert gas through the magnetron and by applying no RF bias to the wafer. The chromium layer is atomically bonded to the microscopically rough wafer surface. A layer of a nickel-vanadium alloy is deposited on the chromium layer and a layer of a metal selected from the group consisting of gold, silver and copper is deposited on the nickel-vanadium layer. The nickel-vanadium layer is deposited between the chromium layer and the metal layer with an intrinsic compressive stress
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a method of etching a surface of a wafer with a microscopic roughness to prepare the wafer surface for receiving a deposition of a material on the wafer surface, the steps of removing a thin layer from the surface of the wafer to eliminate any impurities from the surface of the wafer, wherein the material of the thin layer is the same as the material of the remaining wafer, and thereafter creating the microscopic roughness on the surface of the wafer to receive a deposition of the material on the surface by providing ions of an inert gas by physical RF plasma etch with an insufficient energ
- Claim 2Depends on #1
In a method as set forth in claim 1 wherein the inert gas is argon.
- Claim 3Depends on #1
In a method as set forth in claim 1 where
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (14)
Non-Patent Literature (5)
- "Multilayer Ground Plane Fabrication", Apr. 1, 1969, IBM Technical Disclosure Bulletin, vol. 11, pp. 1596-1597.
- "Pit corrosion inhibition in Sputtered Thin Films", Apr. 1, 1993, IBM Technical Disclosure Bulletin, vol. 36, pp. 405 and 406.
- D.B. Beach, "Design of low-temperature thermal chemical vapor deposition processes", IBM J. REs. Develop., Nov. 1990, vol. 34, No. 6,.
- Valery Felmetsger, "Stress Control in multi-Layer Backside Metallization of Thinned Wafers", Oct. 1999, Sputtered Films, Inc., pp. 1-15.
- Valery Felmetsger, "Tailoring Sputtered Cr Films on Large Wafers", 1999, Sputtered Films, Inc., pp. 1-8.