Patents
US 7,208,203 B2#26411549 Most CitedExpiredUnited States (USPTO)Utility

Method for forming metal oxide film and method for forming secondary electron emission film in gas discharge tube

4Forward Citations (#26411549 Global)
0.2/yrCitation Velocity (#32353261 Global)
1.20Citation PageRank (#31834499 Global)
17Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

According to the present invention, there is provided a method for forming a metal oxide film comprising, when a metal oxide film is formed by conducting a thermal treatment on a coating film containing an organic metal compound formed on an inner wall of a tube, performing an ultraviolet irradiation treatment or an ozone treatment on the coating film prior to or simultaneously with the thermal treatment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming a metal oxide film comprising the steps of: forming a metal oxide film by conducting a thermal treatment on a coating film containing an organic metal compound formed on an inner wall of a tube, and performing an ultraviolet irradiation treatment or an ozone treatment on the coating film prior to or simultaneously with the thermal treatment; wherein the tube has an opening and a length, and wherein the size of the opening is not more than 2 mm and the length is not less than 30 cm.

  2. Claim 2Depends on #1

    The method for forming a metal oxide film of claim 1 , wherein the ultraviolet irradiation treatment or the ozone treatment is performed prior to the thermal treatment and simultaneously with a drying process of the coating film.

  3. Claim 3Depends on #1

    The method for forming a metal oxide film of claim 1 , wherein the step of performing an ultraviole

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (17)

PatentTitleYearCitations
US 3,809,944 ALow-pressure mercury vapour discharge lamp197417
JP S5913605 AManufacture of substrate having thin metallic oxide film—4
US 4,544,997 ALow-pressure mercury vapor discharge lamp198543
US 4,911,953 AProcess for producing composite materials having a coating of calcium phosphate compound199055
US 4,988,661 ASteam reforming catalyst for hydrocarbons and method of producing the catalyst199147
US 5,260,241 AControlled pore size phosphate-alumina material and method for producing same199327
JP H0789720 ACoating liquid for colored film forming, colored film, colored antistatic film and colored low reflective antistatic film—5
US 5,935,638 ASilicon dioxide containing coating199938
US 5,962,079 AUltra thin silicon oxide and metal oxide films and a method for the preparation thereof199977
US 5,995,696 AHollow waveguide and method of making same199964
EP 1,108,468 A1Thin film deposition apparatus—4
US 6,337,032 B1Sol-gel precursor and method for formation of ferroelectric materials for integrated circuits200255
US 6,376,691 B1Metal organic precursors for transparent metal oxide thin films and method of making same200215
US 6,399,145 B1Method for coating lamp bulbs20028
US 6,576,302 B1Method for producing a metal oxide and method for forming a minute pattern200340
US 6,893,677 B2Method for forming coating film on internal surface of elongated tube and unit for forming the same20056
US 6,932,664 B2Gas discharge tube and method for forming electron emission layer in gas discharge tube20055

Non-Patent Literature (1)

  • "Laser Micro-Fabrication of Waveguide Devices", IBM Technical Disclosure Bulletin, vol. 31, #11, Apr. 1, 1989, pp. 150-152.