Method for forming CoWRe alloys by electroless deposition

19Forward Citations (#4550702 Global)
1.0/yrCitation Velocity (#6285720 Global)
3.26Citation PageRank (#6639223 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for fabricating a capping layer with enhanced barrier resistance to both copper and oxygen diffusion, comprises forming a capping layer on a conductive surface of an interconnect, wherein the capping layer comprises cobalt (Co), tungsten (W), rhenium (Re), and at least one of phosphorus (P) and boron (B). In an embodiment of the invention, forming the capping layer comprises exposing the conductive surface to an electroless capping solution comprising a cobalt source, a tungsten source, a rhenium source, and at least one of a phosphorus source and a boron source, and annealing the capping layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 19.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating a capping layer with enhanced barrier properties, comprising: forming a capping layer on a conductive surface of an interconnect, wherein the capping layer comprises cobalt, tungsten, rhenium, calcium, and at least one element selected from the group consisting of phosphorus and boron, and annealing the capping layer.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the capping layer comprises a rhenium concentration of within a range from about 0.1 atomic % to about 10 atomic %.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the rhenium concentration is within a range of from about 0.5 atomic % to about 4 atomic %.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗