Direct coupling of melt polymerization and solid state processing for PET
Abstract
Strands of molten polyethylene terephthalate (PET) from a PET polycondensation reactor are solidified, pelletized, and cooled only to a temperature in the range of 50° C. to a temperature near the polymer Tg by contact with water. The still hot pellets are conveyed, optionally followed by drying to remove water, to a PET crystallizer. By avoiding cooling the amorphous pellets to room temperature with water and cool air, significant savings of energy are realized.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 18.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for decreasing energy usage in a polyethylene terephthalate production process comprising a) solidifying a molten polyethylene terephthalate to form amorphous polyethylene terephthalate pellets and cooling the pellets to a temperature from about 50° C. to about the Tg of the polyethylene terephthalate to form warm polyethylene terephthalate pellets; and b) conveying said warm polyethylene terephthalate pellets to a crystallizer, wherein the temperature of the warm polyethylene terephthalate pellets is in the range of about 50° C. to below the T g of the polyethylene terephthalate at
- Claim 2Depends on #1
The process of claim 1 , wherein said step of conveying comprises introducing said warm pellets into a stream of water having a temperature of between about 50° C. and 90° C.
- Claim 3Depends on #2
The process of claim 2 , wherein prior
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗