Metal plating process
Abstract
A process for forming a coating on a metal substrate includes contacting the substrate with a molybdate solution having a pH of between 3.5 and 5 inclusive containing an acid with the proviso that the acid is not nitric acid. The substrate is contacted with the solution at a temperature between 30 and 75 degrees Celsius and results in a yellow coating that is kinetically stable from 20 seconds to 300 seconds before the coating darkens to a final black coloration. Water washing of the yellow coating precludes further color development. The resulting yellow coating is amenable to overlayering with a seal coat.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for forming a coating on a metal substrate comprising: contacting the substrate with a molybdenum-containing solution having a pH of between 3.5 and 5, inclusive, and containing an acid, with the proviso that the acid is not nitric acid at a temperature between 30 and 75 degrees Celsius such that a yellow coating develops from between 20 and 300 seconds after contact therewith wherein molybdenum is the only metal responsible for the yellow coating and present within said solution as a molybdate or M 0 (VI)Q m X n where X is in each instant independently fluorine, chlorine or bromine
- Claim 2Depends on #1
The process of claim 1 wherein said solution is independent of chromium.
- Claim 3Depends on #1
The process of claim 1 wherein said molybdenum containing solution has a molybdenum ion concen
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (24)
Non-Patent Literature (5)
- Aldoa Technical Bulletin (undated)/Material Safety Data Sheet (Jul. 2001) for Aldokote NCB non chromium black on zinc deposits.
- Aldoa Technical Bulletin (undated)/Material Safety Data Sheet (Oct. 2001) for Aldokote BZN non chromium black on zinc/zinc-nickel alloy plating.
- Derwent abstract of JP 53/016328, Feb. 1978.
- English translation of JP53/016328, Feb. 1978.
- Short et al. "An Investigation into the Oxidation State of Molybdenum in Simplified High Level Nuclear Waste Glass Compositions" (undated).