Method for producing a hole in a body, specifically an injection hole in a fuel injector
Abstract
A method for producing a hole in a body, especially an injection hole in a fuel injector is disclosed. The hole (L) is first produced by a percussion boring process or a trepanation boring process using a laser. The percussion boring process lasts less than 3 seconds. The trepanation boring process lasts less than 10 seconds. After percussion boring or trepanation boring a smoothing step is carried out by forcing a medium that is mixed with abrasive particles under pressure through the hole until any roughnesses of surfaces (F) of the body that form the hole (L) are substantially removed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 11.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for producing an injection hole or throttle in a fuel injector, said method consisting of: percussion drilling the injector at a specific surface location using a laser lasting three seconds or less to form a hardened layer of about 10 μm to about 50 μm thick directly beneath the surface location, performing a smoothing process by forcing a medium containing abrasive particles through the hole or throttle under pressure until a surface unevenness of the wall of the hole or throttle are removed without uncontrolled enlargement of the hole, wherein the smoothing process is performed at
- Claim 2Depends on #1
A method according to claim 1 , wherein the percussion drilling process lasts no longer than 1 s.
- Claim 3Depends on #1
A method according to claim 1 ,
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (11 of 11 total)
References Cited — Backward Prior Art (22)
Non-Patent Literature (3)
- "Diesel Nozzle-the Determining Interface Between Injection system and Combustion Chamber"; D. Potz, W. Christ and B. Dittus; pp. 249-258, 2000.
- "Drilling of Ceramics with Short-Pulsed Solid-State Lasers"; Friedrich Doausinger, Tobias Abeln, et al.; pp. 78-85, 1999.
- "Neue Moglichkeiten der Verbrennungsoptimierung durch hydroerosives Runden von Einspritzdusen"; Dr.-Ing. Detlev Polz et al.; pp. 64-77.