Rotomolding process with reduced cycle times
Abstract
The cycle time for a rotomolding process is improved through the use of a molding material comprising a blend of at least two polyethylenes having narrow molecular weight distributions and homogeneous comonomer distributions. Alternatively, the molding temperature may be reduced to conserve energy and reduce energy costs. The polyethylene blend also has a narrow molecular weight distribution of less than 3 and a density of from 0.930 to 0.950 g/cc. Rotomolded parts prepared from the blend composition have excellent impact resistance and are also resistant to warpage. A preferred process employs a blend composition which contains a blend component having a higher molecular weight and a lower density than another blend component—this blend may be used to prepare rotomolded parts with warpage resistance and improved environmental stress crack resistance (ESCR). A highly preferred process uses a blend composition which further contains a minor amount (from 0.5 to 10 weight %) of a third ethylene blend component which has a higher molecular weight and density—this highly preferred composition may be used to prepare rotomolded parts having warpage resistance, very good ESCR and comparati
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A rotomolding process comprising (i) preparing a polymer blend comprising a plurality of thermoplastic linear ethylene copolymer blend components wherein each blend component has a homogeneous comonomer distribution and a molecular weight distribution, Mw/Mn, of less than 3 and wherein said polymer blend has an overall molecular weight distribution, Mw/Mn, of less than or equal to 3.0 and a density of from 0.930 g/cc to 0.950 g/cc; and (ii) subjecting said polymer blend to rotational molding.
- Claim 2Depends on #1
The process of claim 1 wherein said polymer blend is further characterized by having a density of from 0.935 g/cc to 0.945 g/cc and a melt index, I 2 , of from 1 to 7 grams per 10 minutes.
- Claim 3Depends on #1
The process of claim 1 wherein said polymer blend is further characterized by including at least one third blend component having a higher molecular weight and a higher den
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (15)
Non-Patent Literature (1)
- Anunay Gupta and Urs Stadler, Influence of Stabilizers in Rotational Molding, presented at 22nd Annual Fall Meeting of the Association of Rotational Molders, Oct. 1997, U.S.A.