Cold rolling process for metal tubes

1Forward Citations (#61899224 Global)
0.1/yrCitation Velocity (#54922874 Global)
0.74Citation PageRank (#61899224 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In the cold rolling process by pilger rolling that holds a mandrel between each of paired roll-dies, by optimizing the side relief rate SR and the mandrel factors like the taper θ 1 in the primary deformation zone of the mandrel and the taper θ 2 in the final size reduction zone thereof, and the feed rate F of the workpiece material, and at the same time by properly adjusting the relationship between the side relief rate SR and the feed rate F, the dimension-related shape characteristics (near-perfect round shape) of the tube inside surface after the final finishing rolling process by pilger rolling can be ascertained to thereby ensure excellent surface property without requiring a new apparatus, and further without causing the decrease of the product yield and/or the increase of the manufacturing costs. Thus, this can be widely applied for producing steam generator tubes which exhibits high S/N ratio in the inner coil eddy current testing.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A cold rolling process for metal tubes in which the cold rolling process by pilger rolling that employs a pair of roll-dies with a roll caliber comprising a roll caliber diameter Dx and a side relief amount Fx and holds a mandrel between each of said roll-dies is applied as a final finishing process: wherein a side relief rate SR of said roll-dies expressed by the equation [1] as below is set in the range of 0.5 to 1.5%; wherein said mandrel is configured in such a way that a taper θ 1 in the primary deformation zone of said mandrel is set to 0.25 degree or less, and a taper θ 2 in the final