Patents
US 7,186,663 B2#10334195 Most CitedExpiredUnited States (USPTO)Utility

High density plasma process for silicon thin films

10Forward Citations (#10334195 Global)
0.5/yrCitation Velocity (#14908403 Global)
2.22Citation PageRank (#12265472 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method is provided for forming a Si and Si—Ge thin films. The method comprises: providing a low temperature substrate material of plastic or glass; supplying an atmosphere; performing a high-density (HD) plasma process, such as an HD PECVD process using an inductively coupled plasma (ICP) source; maintaining a substrate temperature of 400 degrees C., or less; and, forming a semiconductor layer overlying the substrate that is made from Si or Si-germanium. The HD PECVD process is capable of depositing Si at a rate of greater than 100 Å per minute. The substrate temperature can be as low as 50 degrees C. Microcrystalline Si, a-Si, or a polycrystalline Si layer can be formed over the substrate. Further, the deposited Si can be either intrinsic or doped. Typically, the supplied atmosphere includes Si and H. For example, an atmosphere can be supplied including SiH4 and H2, or comprising H2 and Silane with H2/Silane ratio in the range of 0–100.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming a semiconductor thin film, the method comprising: providing a substrate; supplying an atmosphere with a hydrogen partial pressure; performing a high-density (HD) plasma enhanced chemical vapor deposition (PECVD) process, connecting a top electrode to an inductively coupled HD plasma source, as follows: locating the substrate between a bottom electrode and the top electrode; supplying a power density in the range of 0 to 10 W/cm 2 , at a frequency in the range of 13.56 to 300 MHz, to the top electrode; and, supplying a power density in the range of 0 to 3 W/cm 2 , at a freq

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • U.S. Appl. No. 60/477,752.