Method of fabricating a semiconductor device utilizing a catalyst material solution
Abstract
A very thin oxide film is formed on an amorphous silicon film that is formed on a glass substrate, and an aqueous solution such as an acetate solution added with a catalyst element such as nickel by 10 to 200 ppm (adjustment needed) is dropped thereon. After the structure is held in this state for a predetermined period, spin drying is performed by using a spinner. A crystalline silicon film is obtained by subjecting the structure to a heat treatment of 550° C. and 4 hours and then to laser light irradiation. A crystalline silicon film having a smaller defect concentration is obtained by further performing a heat treatment of 550° C. and 4 hours.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 6.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of fabricating a semiconductor device comprising: forming a semiconductor film over a substrate having an insulating surface; selectively introducing a material comprising metal for promoting crystallization of the semiconductor film; irradiating the semiconductor film with a laser light to crystallize; after irradiating, annealing the irradiated semiconductor film with a light; and after annealing, patterning the semiconductor film to form at least one semiconductor island.
- Claim 2Depends on #1
A method according to claim 1 wherein said laser light is selected from the group consisting of KrF, XeCl, XeF, and ArF.
- Claim 3Depends on #1
A method according to claim 1 wherein said light is an infrared light.