Patents
US 7,186,480 B2#141058853 Most CitedExpiredUnited States (USPTO)Utility

Method for adjusting dimensions of photomask features

0Forward Citations (#141058853 Global)
0.0/yrCitation Velocity (#141058853 Global)
0.56Citation PageRank (#141058853 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for adjusting one or more dimensions of a photomask subsequent to etching of a defective pattern in the chrome-containing layer thereof is provided. The method includes subjecting the chrome-containing layer of a photomask to a wet etch process utilizing a solution comprising deionized water and ozone. The length of exposure is directly proportional to the degree of adjustment desired. That is, if a small adjustment in one or more dimensions of a photomask is desired, the photomask may be exposed to the deionized water and ozone solution for only a few moments, whereas if a much larger adjustment is necessary, the photomask may be exposed to the solution for several hours. Accordingly, the method of the present invention provides a way in which dimensions of a photomask may be adjusted by a small amount (e.g., a few angstroms) or more severely adjusted, for example, by 20–30 nanometers or more.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for adjusting at least one dimension of a photomask, comprising: providing a photomask having a chrome-containing layer disposed over a silicon oxide-containing substrate, the photomask including at least one feature in the chrome-containing layer thereof which has a first dimension; and subjecting the photomask to a solution consisting essentially of deionized water and ozone for a period of time sufficient to adjust the first dimension of the at least one feature in the chrome-containing layer to a second dimension more closely approximating a desirable value than the first dimensio

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the at least one dimension of the photomask is a critical dimension.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein subjecting the photomask to a solution consisting essentially of deionized water and ozone comprises subject

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • Buie et al., "Chrome Etch for <0.13 um Advanced Reticle Production," Applied Materials Photomask Etch, Sunnyvale, CA., date unknown, pp. 1-8.