Process for producing hydrophobic silica powder
Abstract
A process for producing a hydrophobic silica powder, comprises the steps for hydrophobic treatment of: adding to a silica sol in mixed solvent having a silica concentration of 5 to 50 mass % obtained by mixing an aqueous silica sol containing hydrophilic colloidal silica having a specific surface area of 5.5 to 550 m 2 /g with a hydrophilic organic solvent in a mass ratio of 0.12 to 2.5 based on water in the aqueous silica sol, a disilazane compound of formula (1) (R 1 3 Si) 2 NH (1) wherein each R 1 is C 1-6 alkyl group or phenyl group that is selected independently of one another, in an amount of 0.1 to 20 mmol per surface area 100 m 2 of the hydrophilic colloidal silica, to obtain a mixture of the silica sol in mixed solvent and the disilazane compound; and heating the mixture at a temperature of 50 to 100° C. for aging it to obtain a slurry dispersion of hydrophobic treated colloidal silica. The process provides a hydrophobic silica powder through a simple hydrophobic treatment step.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing a hydrophobic silica powder comprising the steps for hydrophobic treatment of: adding to a silica sol in mixed solvent having a silica concentration of 5 to 50 mass % obtained by mixing an aqueous silica sol containing hydrophilic colloidal silica having a specific surface area of 5.5 to 550 m 2 /g with a hydrophilic organic solvent in a mass ratio of 0.12 to 2.5 based on water in the aqueous silica sol, a disilazane compound of formula (1) (R 1 3 Si) 2 NH (1) wherein each R 1 is C 1-6 alkyl group or phenyl group that is selected independently of one another, in an
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗