A copper-base alloy with increased melting point above 1000° C., which is resistant or immune to carburization, metal dusting and coking, resistant to oxidation at elevated temperatures. The alloy has the following composition (in weight-%): Al 4–15, Si 0.1–6, Mo 0.5–40, W 0–40, where the total of Mo and W do not exceed 40%, one or more of the group of Rare Earth Metals (REM), such as yttrium, hafnium, zirconium, lanthanum and/or cerium, up to 1.0 weight-% of each element or a total of maximum 3.0 weight-%, Cu balance and normally occurring alloying additions and impurities. A method for the alloy's production, and the alloy's use as construction components in CO-containing atmospheres, ammonia containing atmospheres, and/or hydrocarbon containing atmospheres or solid carbon containing processes, are also disclosed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A copper-base alloy having a melting point of at least 1000° C. and a composition comprising, in weight-%: Al 4–15; Si 0.1–6; Mo 10–40; W 0–40, wherein the total of Mo and W does not exceed 40 weight-%; one or more elements selected from the group consisting of Rare Earth Metals, hafnium and zirconium in an amount up to 1.0 weight-% of each element or a total amount of a maximum 3.0 weight-%; Cu balance; and normally occurring alloying additions and impurities, wherein the melting point is at least 1100° C.

  2. Claim 2Depends on #1

    The copper-base alloy according to claim 1 , wherein the melting point is at least 1200° C. and the composition comprises in weight-%: Mo 22–40.

  3. Claim 3Depends on #2

    The copper-base alloy according to claim 2 , wherein the melting point is at least 1300° C. and the composition comprises, in weight-%: Mo 40.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

PatentTitleYearCitations
US 2011059335 A1Composite Tube—6

Non-Patent Literature (2)

  • "Phase Diagrams of Binary Alloy Systems", Metals Handbook, 8<SUP>th </SUP>Ed., vol. 8, Metallography, Structures and Phase Diagrams, American Society for Metals, Metals Park, Ohio, 1973, p. 259.
  • Lundberg et al., U.S. Appl. No. 10/921,943, filed Aug. 20, 2004 entitled "Metal Dusting Resistant Product".