Method of making ceramic composite devices with unidirectionally aligned reinforcing fibers
Abstract
Ceramic composite materials have unidirectional alignment of the reinforcing fibers. The ratio of the volume of the fiber strands of the reinforcing fibers to the volume of the matrix is at least 0.5. A process for their production involves initially coating the fiber strands or rovings of the reinforcing fibers with a sacrificial polymer. The coated fiber strands are processed with binder resins into unidirectionally reinforced CFK molded parts. The formed CFK bodies are carbonized to form CFC bodies. The CFC bodies are then silicized with liquid silicon. The liquid silicon diffuses into the pores formed in the CFC body and combines there at least partially with the carbon to form silicon carbide. The sacrificial polymer is pyrolized. The ceramic composite materials also can be used in fiber-reinforced ceramic structural parts.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 11.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing ceramic composite materials with unidirectionally aligned reinforcing fibers, which comprises: providing a polymer over reinforcing fibers, the polymer having a mass; processing the reinforcing fibers having the polymer thereover by adding binder resins to form a unidirectionally reinforced CFK molded part; carbonizing the unidirectionally reinforced CFK molded part to form a Carbon Fiber-reinforced Carbon (CFC) body; decomposing the polymer at least almost completely during the carbonizing step to form a carbon residue in an amount of up to 60% of the mass of the polym
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗