High-density plasma (HDP) chemical vapor deposition (CVD) methods and methods of fabricating semiconductor devices employing the same
Abstract
In one embodiment, a semiconductor substrate is placed into a process chamber. A gas mixture including a silicon-containing gas, a fluorine-containing gas, an inert gas, and an oxygen gas is introduced into the chamber at a pressure range of from about 30 mTorr to about 90 mTorr. During this time, deposition and etching processes are concurrently performed using a plasma to form a high-density plasma (HDP) insulating layer on the semiconductor substrate. A ratio of deposition to etching is from about 3:1 to about 10:1. A ratio of a flow rate of the fluorine-containing gas to a flow rate of the silicon-containing gas is less than about 0.9.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of manufacturing a semiconductor device, the method comprising: placing a semiconductor substrate with a trench in a chamber; forming a first insulating layer on a bottom of the trench; concurrently performing deposition and etching processes to form a gap-fill dielectric layer over the first insulating layer by introducing a gas mixture comprising a silicon-containing gas, a fluorine-containing gas, an inert gas, an oxygen gas, and also a hydrogen gas into the chamber under a high-density plasma condition at a pressure range of from about 30 mTorr to about 90 mTorr, wherein a ratio o
- Claim 2Depends on #1
The method of claim 1 , which further comprises forming a second insulating layer over the dielectric layer.
- Claim 3Depends on #1
The method of claim 1 , where
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (9)
Non-Patent Literature (1)
- Jörg Radecker, et al. "Extending the HDP-CVD Technology to the 90nm Node and Beyond with an In-Situ Etch Assisted (ISEA) HDP-CVD Process" IEEE, 2003 pp. 125-130.