Patents
US 7,183,186 B2#14484099 Most CitedExpiredUnited States (USPTO)Utility

Atomic layer deposited ZrTiO4 films

7Forward Citations (#14484099 Global)
0.4/yrCitation Velocity (#21687687 Global)
2.35Citation PageRank (#11255630 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

After pulsing the second purging gas, a zirconium-containing precursor is pulsed into reaction chamber 220, at block 430. In an embodiment, the zirconium-containing precursor is ZTB. In other embodiments, a zirconium-containing precursor includes but is not limited to ZrCl<SUB>4 </SUB>and ZrI<SUB>4</SUB>. The ZTB precursor is pulsed into reaction chamber 220 through the gas-distribution fixture 240 on substrate 210. Mass-flow controller 258 regulates the flow of the ZTB from gas source 253. In an embodiment, the substrate temperature is maintained at about 200° C. The ZTB aggressively reacts at the current surface of substrate 210.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a film comprising: pulsing a titanium-containing precursor onto a substrate; pulsing a zirconium tertiary-butoxide precursor to form a film containing ZrTiO 4 by atomic layer deposition; and forming a dielectic barrier layer by atomic layer deposition, the dielectric barrier layer being a non-oxygen containing material formed between and contacting the substrate and the film.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the method further includes controlling the pulsing of the titanium-containing precursor and the pulsing of the zirconium tertiary-butoxide precursor to provide the film with a predetermined ratio of Zr to Ti.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein pulsing a titanium-containing precursor includes pulsing a titanium-containing precursor selected from a group consisting of TiCl 4 ,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,058,430 AMethod for producing compound thin films19771,251
US 5,055,319 AControlled high rate deposition of metal oxide films199186
EP 0,540,993 A1Structure and fabrication of high transconductance MOS field effect transistor using a buffer layer/ferroelectric/buffer layer stack as the gate dielectric—73
US 5,302,461 ADielectric films for use in magnetoresistive transducers199462
US 5,572,052 AElectronic device using zirconate titanate and barium titanate ferroelectrics in insulating layer1996177
US 5,621,681 ADevice and manufacturing method for a ferroelectric memory199789
US 5,625,233 AThin film multi-layer oxygen diffusion barrier consisting of refractory metal, refractory metal aluminide, and aluminum oxide199793
US 5,674,563 AMethod for ferroelectric thin film production199769
US 5,744,374 ADevice and manufacturing method for a ferroelectric memory199872
US 5,751,021 ASemiconductor light-emitting device199869
US 5,795,808 AMethod for forming shallow junction for semiconductor device1998108
US 5,801,105 AMultilayer thin film, substrate for electronic device, electronic device, and preparation of multilayer oxide thin film1998157
US 5,810,923 AMethod for forming oxide thin film and the treatment of silicon substrate1998149
US 5,828,080 AOxide thin film, electronic device substrate and electronic device1998160
US 5,840,897 AMetal complex source reagents for chemical vapor deposition1998230
US 5,912,797 ADielectric materials of amorphous compositions and devices employing same199968
US 5,916,365 ASequential chemical vapor deposition1999819
US 6,010,969 AMethod of depositing films on semiconductor devices by using carboxylate complexes2000135
US 6,020,024 AMethod for forming high dielectric constant metal oxides2000398
US 6,027,961 ACMOS semiconductor devices and method of formation2000301
US 6,093,944 ADielectric materials of amorphous compositions of TI-O2 doped with rare earth elements and devices employing same200076
US 6,110,529 AMethod of forming metal films on a substrate by chemical vapor deposition2000207
US 6,171,900 B1CVD Ta2O5/oxynitride stacked gate insulator with TiN gate electrode for sub-quarter micron MOSFET2001129