Patents
US 7,178,366 B2#15659869 Most CitedExpiredUnited States (USPTO)Utility

Method for the production of an internally vitrified SiO2 crucible

7Forward Citations (#15659869 Global)
0.4/yrCitation Velocity (#21737230 Global)
1.59Citation PageRank (#20811805 Global)
4Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for producing an SiO 2 shaped body which is at least partially vitrified, wherein an amorphous, porous SiO 2 green body is sintered or vitrified by contactless heating by means of radiation, while avoiding contamination to the SiO 2 shaped body with foreign atoms, wherein the radiation used is the beam of a laser at a subatmospheric pressure below 1000 mbar.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 7.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for the production of a crack-free, internally vitrified SiO 2 crucible, comprising: sintering an amorphous, open-pored SiO 2 green-body crucible by means of exposure to a focal spot of a CO 2 laser beam, wherein the focal spot is moved relative to the inner surface of said crucible throughout the sintering, the sintering beginning at an upper inner edge of the SiO 2 green-body crucible by means of a focal spot of a first contact area, the focal spot sweeping over the upper inner edge of the SiO 2 green-body crucible and broadening during said sweeping to a second, larger contact

  2. Claim 2Independent Claim

    The method

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • English Derwent Abstract [AN 2003-532490] [50] corresponding to DE 101 58 521 A1.
  • English translation corresponding to patent application DE 102 60 320.