Abstract
A jettable non-curable support material composition useful for three-dimensional ink jet printing comprising at least one fatty alcohol and at least one abietic rosin ester alcohol, wherein the support material has a melting point between about 50° C. to about 65° C. and a freezing point between about 45° C. to about 55° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 12.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A non-curable support material composition useful for three-dimensional ink jet printing to help create a part formed from a build material, the non-curable support material consisting of at least one jettable fatty alcohol of the structure C n H 2n+1 OH having a melting point between about 50° C. to about 65° C. and a freezing point between about 45° C. to about 55° C. and a jettable rosin ester, the support material composition having a melting point higher than uncured build material used to form the part and a viscosity at about 80° C. from about 10.0 to about 19.0 centipoise.
- Claim 2Depends on #1
The composition of claim 1 wherein the fatty alcohol is from about 60% to about 80% by weight of the composition.
- Claim 3Depends on #2
The composition of claim 2 wherein the rosin ester is from about 20% to about 40% by weight of the composition.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (17)
Non-Patent Literature (1)
- Lewis Sr., Richard J.; Sax's Dangerous Properties of Industrial Materials 10th Ed., John Wiley & Sons, NY (2000).