Method for the repair of defects in photolithographic masks for patterning semiconductor wafers
Abstract
A method for repairing defects in a photolithographic mask for use in patterning semiconductor wafers introduces a pre-selected phase error selected to sum with a phase error of a defect repair material, yielding a desired composite phase error relative to light passing through the substrate alone, e.g., 180°. Substrate phase error may be introduced by modifying its thickness. For example, after any opaque layer material within a repair zone surrounding the defect is removed, the substrate, too, is removed within the repair zone to a pre-selected depth, forming a lacuna. Repair material is then deposited in the lacuna and in the remainder of the repair zone to a level substantially equal to the top surface of the opaque layer, yielding a desired, combined phase error and attenuation matching those of defect free regions of the mask where the opaque layer has not been removed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for repairing a defect in a photolithographic mask for semiconductor patterning, the photolithographic mask having a substrate or first layer of a first material with a first thickness and a first light transmittance and a second layer of a second material having a second light transmittance differing from the first, the second layer being removable in at least one pre-selected region to form a pattern, the second layer, when intact, causing a selected phase shift in light waves that pass through it relative to light passing through the first layer or substrate alone, and, when absent
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗