Patents
US 7,150,786 B2#4998560 Most CitedExpiredUnited States (USPTO)Utility

Very early setting ultra-high strength cement

18Forward Citations (#4998560 Global)
0.9/yrCitation Velocity (#7939578 Global)
2.52Citation PageRank (#10020180 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Clinkered materials containing high concentrations of {(C,K,N,M) 4 (A,F,Mn,P,T,S) 3 (cl,{overscore (S)})} (crystal X), and {(C 2 S) 3 (C{overscore (S)}) 3 Ca(f,cl) 2 } or {(C 2 S) 3 (C{overscore (S)}) 3 Ca(f,cl) 2 } (crystal Y), and/or {C 5 S 2 {overscore (S)}) (crystal Z) directly from the kiln, rapidly hardening ultra-high early strength cement including these clinkered materials, methods for forming and using said compositions and the cements so produced are claimed. The methods include the steps of forming a mixture of raw material containing CaO, MgO, Al 2 O 3 , Fe 2 O 3 , TiO 2 , Mn 2 O 3 , SiO 2 , SO 3 , Na 2 O, K 2 O, P 2 O 5 and F, respectively designated C, M, A, F, T, Mn, S, {overscore (S)}, N, K, P and f, and heating said mixture to an elevated temperature between 900° C. and 1,200° C.; before determining average amount of crystals X, Y, and Z. Final mixtures comprising these clinkers and hydraulic or portland type cement are made to produce cement compositions having crystal X concentrations of approximately 5% to 35% by weight, crystal Y concentrations of approximately 5% to 40% by weight, and/or crystal Z concentrations of approximately 5% to 40% by weight, with the

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 18.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A cement comprising a clinkered material, the clinkered material comprising a crystal having the solid solution formula {(C,K,N,M) 4 (A,F,Mn,P,T,S) 3 (cl,{overscore (S)})} and a crystal having the solid solution formula {(C 2 S) 3 (C{overscore (S)}) 3 Ca(f,cl) 2 }.

  2. Claim 2Depends on #1

    The cement of claim 1 , further comprising CaO.

  3. Claim 3Depends on #1

    The cement of claim 1 having a compressive strength greater than 3,000 psi within approximately one hour following hydration.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • Cesare Gilioli, Franco Massazza and Mario Pezzuoli, "A New Compound Containing Five Components: 17.2Ca0.0.8K<SUB>2</SUB>0.6Si0<SUB>2</SUB>.3S0<SUB>3</SUB>.CaF<SUB>2</SUB>," Cement and Concrete Research, vol. 9, pp. 695-699, 1979, Copyright (C) 1979 Pergamon Press, Ltd.
  • S. Gimenez-Molina and M.T. Blanco-Varela, "Solid State Phases Relationship In The CaO-SiO<SUB>2</SUB>-A1<SUB>2</SUB>O<SUB>3</SUB>-CaF<SUB>2</SUB>-CaSO<SUB>4 </SUB>System," Cement and Concrete Research, vol. 25 No. 4, pp. 870-882, 1995, Copyright (C) 1995 Elsevier Science Ltd.
  • Y. Pliego-Cuervo and F.P. Glasser, "Phase Relations and Crystal Chemistry of Apatite and Silicocarnotite Solid Solutions," Cement and Concrete Research, vol. 8, pp. 519-524, 1978, Pergamon Press, Inc.