Patents
US 7,149,074 B2#25149062 Most CitedExpiredUnited States (USPTO)Utility

Methods of making a niobium metal oxide

4Forward Citations (#25149062 Global)
0.2/yrCitation Velocity (#32810450 Global)
1.33Citation PageRank (#27416082 Global)
46Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Methods to at least partially reduce a niobium oxide are described wherein the process includes heat treating the niobium oxide in the presence of a getter material and in an atmosphere which permits the transfer of oxygen atoms from the niobium oxide to the getter material, and for a sufficient time and at a sufficient temperature to form an oxygen reduced niobium oxide. Niobium oxides and/or suboxides are also described as well as capacitors containing anodes made from the niobium oxides and suboxides.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 46 · Forward citations: 4.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming a capacitor anode comprising a niobium oxide having an atomic ratio of niobium to oxygen of 1:less than 2.5, comprising forming said niobium oxide into the shape of an anode and sintering at a temperature of from about 800° C. to about 1200° C. for a time of from about 1 hour to about 10 hours; anodizing at from about 16 to about 75 volts at a formation temperature of about 85° C.; annealing said anode at a temperature of from about 300 to about 350° C. for a time of from about 10 minutes to about 60 minutes; and manganizing said anode at a temperature of from about 220° to

  2. Claim 2Independent Claim

    A method of forming a capacitor anode comprising a niobium oxide having an atomic ratio of niobium to oxygen of 1:less than 2.5, comprising forming said niobium oxide into the shape of an anode and sintering at a temperature of from about 800° C. to about 12

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (46)

PatentTitleYearCitations
GB 1,123,015 AA process for producing sintered anodes—27
US 3,962,715 AHigh-speed, high-current spike suppressor and method for fabricating same197627
US 4,118,727 AMOX multi-layer switching device comprising niobium oxide197841
US 4,668,501 AProcess for preparing a titanium oxide powder198749
US 4,805,074 ASolid electrolytic capacitor, and method of manufacturing same198989
US 4,960,471 AControlling the oxygen content in tantalum material199068
US 4,964,906 AMethod for controlling the oxygen content of tantalum material199066
US 5,011,742 AArticle for controlling the oxygen content in tantalum material199124
US 5,032,377 AChromium oxide green, a process for its production and its use199119
US 5,211,741 AFlaked tantalum powder1993104
US 5,245,514 AExtruded capacitor electrode and method of making the same199385
US 5,281,496 AElectrochemical cell containing a titanium suboxide electrode199473
US 5,320,782 AAcicular or platy titanium suboxides and process for producing same199425
EP 0,634,761 A1A method for producing a solid electrolytic capacitor—19
EP 0,634,762 A1A method for producing a solid electrolytic capacitor—12
US 5,412,533 ASolid electrolytic capacitor and manufacturing method thereof199568
US 5,688,730 AOptically transparent gamma-aluminum oxynitride powders and ceramic articles shaped therefrom199721
WO 9,819,811 A1Niobium powders and niobium electrolytic capacitors—73
WO 9,830,348 A1Binder removal—12
US 6,001,281 APreparation of conductive polymers from stabilized precursor solutions199970
DE 19,831,280 A1Acidic earth metal, specifically tantalum or niobium, powder for use, e.g., in capacitor production is produced by two-stage reduction of the pentoxide using hydrogen as the first stage reducing agent for initial suboxide formation—30
WO 0,012,783 A2Phosphate anodizing electrolyte and its use to prepare capacitors valve metal anodes produced from very fine metal powders—7
WO 0,014,139 A1Preparation of conductive polymers from stabilized precursor solutions—11
WO 0,014,755 A1Process of preparing a solid electrolytic capacitor containing a conductive polymer counter electrode—3
WO 0,015,555 A1Methods to partially reduce a niobium metal oxide and oxygen reduced niobium oxides—56
WO 0,015,556 A1Methods to partially reduce certain metal oxides and oxygen reduced metal oxides—25

Non-Patent Literature (5)

  • Andersson, "Die Bedentung des Tantals in der Kondensatorindustrie," Erzmetall, vol. 48, No. 6/7, pp. 430-434 (1995).
  • Baba et al., "Preparation and Chlorination of NbO<SUB>2</SUB>, NbO and NbC," Journal Mining and Mettallurgical Institute of Japan, vol. 82, No. 942, pp. 855-860 (1966).
  • Bauer, "The Oxides of Niobium," Zeitschrift fuer anorganische und allgemeine Chemie, vol. 248, No. 1, pp. 15-45 (1941) (English translation).
  • Brauer et al., "Die Nitride des Niobs," Z. anorg. Allg. Chemie, vol. 270, pp. 160-178 (1952) w/ partial Engl. Trans.
  • Brauer et al., "Mikrokristallines NbO," p. 1462, from Handbuch Der Praparativen Anorganischen Chemie w/ partial English translation.