Alkaline cell with improved anode
Abstract
A method of forming an anode comprising zinc for an alkaline cell. The method involves mixing zinc particles with binders including preferably polyvinylalcohol, surfactant and water to form a wet paste. The wet paste is molded into the near shape of the cell's anode cavity and then heated to evaporate water. A solid porous zinc mass is formed having microscopic void spaces between the zinc particles. The solid mass can be inserted into the cell's anode cavity and aqueous alkaline electrolyte, preferably comprising potassium hydroxide, then added. The solid mass absorbs the aqueous electrolyte and expands to fill the anode cavity to form the final fresh anode.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 7.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming an anode for an alkaline cell having an anode cavity therein, comprising the step of: a) forming a wet mixture comprising zinc particles, a binder comprising polyvinylalcohol and a gelling agent, and water; a.1) inserting said wet mixture into a mold cavity; a.2) applying pressure to said wet mixture in said mold cavity thereby compacting said wet mixture within said mold cavity; a.3) ejecting said compacted wet mixture from said mold cavity thereby producing a molded wet mixture having a molded shape, whereupon said molded wet mixture retains its molded shape; b) drying sa
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗