Piercing method for manufacturing of seamless pipe
Abstract
A piercing method for manufacturing a seamless pipe capable of suppressing the rotary forging effects and suppressing the redundant shear strain without excessive narrowing of the roll diameter is provided. This method is characterized by holding a feed angle β and a cross angle γ of main rolls in a range satisfying the following expressions (1) to (3), setting the relationship between outer diameter “d 0 ” of the solid billet and the outer diameter “d” and thickness “t” of a hollow piece after piercing so as to satisfy the following expression (4), and further setting the relationship between inlet diameter D 1 and outlet diameter D 2 of the main roll with the above-mentioned “d 0 ”, “d” and γ so as to satisfy the following expression (5) 8°≦β≦20° (1) 5°≦γ≦35° (2) 15°≦β+γ≦50° (3) 1.5≦−ψ r /ψ θ ≦4.5 (4) ( d/d 0 )/(0.75+0.025γ)≦ D 2 /D 1 (5) In the expression (4), ψ r =1n(2t/d 0 ) and ψ θ =1n{2(d−t)/d 0 }.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 11.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
5≦−ψ r /ψ θ ≦4.5 (4) ( d/d 0 )/(0.75+0.025γ)≦ D 2 /D 1 (5) In the expression (4), ψ r 1n(2t/d 0 ) and ψ θ =1n{2(d−t)/d 0 }.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗