Patents
US 7,144,837 B2#2316360 Most CitedExpiredUnited States (USPTO)Utility

Clear glass composition with high visible transmittance

30Forward Citations (#2316360 Global)
1.5/yrCitation Velocity (#3448314 Global)
2.84Citation PageRank (#8284355 Global)
28Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A high transmittance fairly clear/neutral colored glass composition is provided. An oxidizing agent(s) such as cerium oxide (e.g., CeO 2 ) or the like is added to the glass batch in order to realize very oxidized conditions (i.e., to significantly lower the redox of the resulting glass). As a result of the oxidizing agent(s) used in the batch, the iron is oxidized to a very low FeO (ferrous state) content. For example, this may result in a glass having a glass redox value of no greater than 0.12 (more preferably <=0.10; even more preferably <=0.08; and most preferably <=0.05) and a % FeO (i.e., ferrous content) of from 0.0001 to 0.05%. In certain example embodiments, in order to compensate for yellow or yellow-green coloration a small amount of cobalt (Co) may be provided in the glass to enable it to realize a more neutral color.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 30.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A glass comprising: a base glass portion comprising (by weight percentage): SiO 2 67 to 75% Na 2 O 10 to 20% CaO 5 to 15% MgO 0 to 8% Al 2 O 3 0 to 5% K 2 O 0 to 5%

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • "Ultraviolet-Absorbing Colorless Transparent Glass", Hidetoshi, JP11060269, vol. 1999, No. 88.