Patents
US 7,144,810 B2#34036216 Most CitedExpiredUnited States (USPTO)Utility

Methods for forming rough ruthenium-containing layers and structures/methods using same

3Forward Citations (#34036216 Global)
0.1/yrCitation Velocity (#38941745 Global)
0.96Citation PageRank (#44396415 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for forming a rough ruthenium-containing layer on the surface of a substrate assembly includes providing a ruthenium-containing precursor into the reaction chamber. A rough ruthenium layer may be deposited on the surface of the substrate assembly at a rate of about 100 Å/minute to about 500 Å/minute using the ruthenium-containing precursor. Further, a rough ruthenium oxide layer may be formed by providing a ruthenium-containing precursor and an oxygen-containing precursor into the reaction chamber to deposit the rough ruthenium oxide layer on the surface of the substrate assembly at a rate of about 100 Å/minute to about 1200 Å/minute. An anneal of the layers may be performed to further increase the roughness. In addition, conductive structures including a rough ruthenium layer or a rough ruthenium oxide layer are provided. Such layers may be used in conjunction with non-rough ruthenium and/or non-rough ruthenium oxide layers to form conductive structures. For example, such structures may be part of a capacitor structure, e.g., bottom electrode of a capacitor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a conductive structure comprising: forming non-rough ruthenium-containing material at a first deposition rate; and forming rough ruthenium-containing material on the non-rough ruthenium-containing material at a second deposition rate, wherein the second deposition rate is greater than the first deposition rate, wherein the rough ruthenium-containing material forms at least a part of a lower electrode of a capacitor, and further wherein a dielectric material is formed on the rough ruthenium-containing material.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the rough ruthenium-containing material is formed of ruthenium and the non-rough ruthenium-containing material is formed of ruthenium.

  3. Claim 3Depends on #1

    The conductive structure of claim 1 , wherein the rough ruthenium-containing material is formed of ruthenium oxide and the non-rough ruthenium-containing

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,953,989 AGas bearing part, and device provided with such a gas bearing part19908
US 5,068,199 AMethod for anodizing a polysilicon layer lower capacitor plate of a DRAM to increase capacitance1991106
US 5,130,172 ALow temperature organometallic deposition of metals1992252
US 5,130,885 ADram cell in which a silicon-germanium alloy layer having a rough surface morphology is utilized for a capacitive surface1992108
US 5,270,241 AOptimized container stacked capacitor DRAM cell utilizing sacrificial oxide deposition and chemical mechanical polishing1993232
US 5,314,727 AChemical vapor deposition of iron, ruthenium, and osmium199463
US 5,318,920 AMethod for manufacturing a capacitor having a rough electrode surface199485
US 5,342,800 AMethod of making memory cell capacitor199471
US 5,352,488 AChemical vapor deposition process employing metal pentadienyl complexes199455
US 5,372,962 AMethod of making a semiconductor integrated circuit device having a capacitor with a porous surface of an electrode1994106
US 5,372,849 AChemical vapor deposition of iron, ruthenium, and osmium1994170
US 5,392,189 ACapacitor compatible with high dielectric constant materials having two independent insulative layers and the method for forming same1995333
US 5,427,974 AMethod for forming a capacitor in a DRAM cell using a rough overlayer of tungsten199536
US 5,510,651 ASemiconductor device having a reducing/oxidizing conductive material1996169
US 5,520,992 AElectrodes for high dielectric constant materials199681
US 5,555,486 AHybrid metal/metal oxide electrodes for ferroelectric capacitors1996204
US 5,561,307 AFerroelectric integrated circuit1996181
US 5,566,045 AHigh-dielectric-constant material electrodes comprising thin platinum layers1996151
US 5,581,436 AHigh-dielectric-constant material electrodes comprising thin platinum layers1996129
US 5,608,247 AStorage capacitor structures using CVD tin on hemispherical grain silicon1997103
US 5,612,560 AElectrode structure for ferroelectric capacitors for integrated circuits199760
US 5,696,014 AMethod for increasing capacitance of an HSG rugged capacitor using a phosphine rich oxidation and subsequent wet etch199757
US 5,763,633 AMetal carboxylate complexes for formation of metal-containing films on semiconductor devices199839
JP H10163131 AMethod of forming ruthenium oxide film and method of manufacturing semiconductor device—17
US 5,874,364 AThin film deposition method, capacitor device and method for fabricating the same, and semiconductor device and method for fabricating the same199981
US 5,877,063 AMethod of forming rough polysilicon surfaces199933
US 5,935,648 AHigh surface area molybdenum nitride electrodes199912

Non-Patent Literature (5)

  • Anderson et al., "Carborane Complexes of Ruthenium: A Convenient Synthesis of [Ru(CO)<SUB>3</SUB>(eta<SUP>3</SUP>-7,8-C<SUB>2</SUB>B<SUB>y</SUB>H<SUB>11</SUB>)] and a Study of Reactions of This Complex," Organometallics, 14, 3516-3526 (1995).
  • Aoyama et al., "Chemical Vapor Deposition of Ru and Its Application in (Ba,Sr)TiO<SUB>3 </SUB>Capacitors for Future Dynamic Random Access Memories,"Jpn. J. Appl. Phys., 38: 2194-2199 (1999).
  • Bai et al., "Low-temperature growth and orientational control in RuO<SUB>2 </SUB>thin films by metal-organic chemical vapor deposition", Thin Solid Films, 310, 75-80 (1997).
  • Bennett et al., "Mono-olefin Chelate Complexes of Iron(0) and Ruthenium(0) with an Olefinic Tertiary Phosphine," J. Chem. Soc. D., 7, 341-342 (1971).
  • Cowles et al., "Relative Reactivity of Co-ordinated Ligands inthe Dienyltricarbonyl-ruthenium Cation, [(dienyl)Ru(CO)<SUB>3</SUB>]<SUP>+</SUP>, " Chemical Commun., 392 (1969).