Patents
US 7,144,547 B2#3859688 Most CitedExpiredUnited States (USPTO)Utility

Target for cathode discharging arc ion plating and method of manufacturing the same

21Forward Citations (#3859688 Global)
1.1/yrCitation Velocity (#6084757 Global)
4.76Citation PageRank (#3585973 Global)
6Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In a target for cathode discharging arc ion plating containing Al and Cr as an essential ingredient according to the invention, the thickness of the Al and Cr compound layer formed between Cr particles and Al contained in a target is 30 μm or less. Alternatively, the total for the peak intensities of Al—Cr compound observed between diffraction angles between 10 to 80° by X-ray diffractiometry according to θ=2θ method is 10% or less relative to the total for the peak intensities of Al, Cr and the Al—Cr compound. Further, the relative density of the target is 92% or more. The target is capable of forming hard films of high quality while preventing not uniform movement of arc spots and suppressing formation of macro particles.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 21.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a target for cathode discharging arc ion plating, comprising: sintering a powder mixture of elements forming the target by a HIP method in which a processing temperature is 420° C. to 485° C.; wherein said target comprises Al and Cr, wherein the thickness of a compound layer of Al and Cr formed between Cr particles and Al contained in the target is 5 μm or less, and wherein the relative density of the target is 92% or more.

  2. Claim 2Independent Claim

    A method of manufacturing a target for cathode discharging arc ion plating, comprising: sintering a powder mixture of elements forming the target by a HIP method in which the processing temperature is 420° C. to lower than 485° C.; wherein said target comprises Al and Cr, wherein the thickness of a compound layer of Al and Cr formed between Cr particles and Al contained in the target is 5 μm or less

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 21 total)

PatentTitleYearCitations
US 7,601,440 B2Hard coating excellent in wear resistance and in oxidation resistance and target for forming the same20092
KR 101,011,549 B1Hard coating having excellent wear resistance and oxidation resistance and target for forming the same, and hard coating having excellent high-temperature lubricating ability and wear resistance and target for forming the same20110
US 7,851,075 B2Work piece with a hard film of ALCR-containing material, and process for its production20104
US 7,592,061 B1Hard coating film20095
US 2009136727 A1Hard coating excellent in wear resistance and in oxidation resistance and target for forming the same—4
US 2009169847 A1Hard films and sputtering targets for the deposition thereof—0
US 2006068225 A1Hard coating excellent in wear resistance and in oxidation resistance and target for forming the same—14
US 7,521,131 B2Hard coating excellent in wear resistance and in oxidation resistance and target for forming the same200928
US 9,611,538 B2Method for producing metal oxide layers through arc vaporization20170
US 2009269600 A1Method for producing metal oxide layers through arc vaporization—22
US 7,988,832 B2Work piece with a hard film of AlCr-containing material, and process for its production20113
KR 100,937,072 B1Hard coating having excellent wear resistance and oxidation resistance and target for forming the same, and hard coating having excellent high-temperature lubricating ability and wear resistance and target for forming the same20100
US 2009246497 A1Hard coating film—0
US 7,510,608 B2Hard coating film20090
US 10,323,320 B2Method for producing metal oxide layers of predetermined structure through arc vaporization20190

Non-Patent Literature (2)

  • Patent Abstracts of Japan, JP 10-060636, Mar. 3, 1998.
  • Patent Abstracts of Japan, JP 2000-297365, Oct. 24, 2000.