Patents
US 7,144,526 B2#43282199 Most CitedExpiredUnited States (USPTO)Utility

Conductive primer composition for ambient cure

2Forward Citations (#43282199 Global)
0.1/yrCitation Velocity (#45773118 Global)
0.94Citation PageRank (#45773560 Global)
15Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention provides electrically conductive and flexible primer compositions that harden to form conductive materials under room temperature or low bake temperature curing conditions. The primer composition contains solvents and 40–75% by weight of film forming binder and pigments in an overall pigment to binder weight ratio of about 1:100 to 100:100; wherein the binder contains (A) a flexible hydroxy containing polyester resin and (B) an organic polyisocyanate crosslinking agent; and wherein the pigments include electrically conductive pigments in a pigment to binder weight ratio of about 1:100 to 130:100 and the electrically conductive pigments consists essentially of a combination of graphite and conductive carbon black pigments in a graphite to carbon black weight ratio of about 120:1 to 1:1, and the composition forms a hard, flexible coating having a surface conductivity of at least 100 Ransburg units when cured at room temperature or low bake conditions. The coating composition can be used on metal or plastic substrates to render the substrate conductive.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A flexible conductive primer coating composition containing solvents and 40–75% by weight of film forming binder and pigments in an overall pigment to binder weight ratio of about 1:100 to 200:100; wherein the binder comprises (A) a polyester copolymer having linear segment with hydroxyl groups that has a hydroxyl number of about 15–300 and a number average molecular weight of about 300–3,000 and branched segments that have hydroxyl groups and have a hydroxyl number of about 175–300 and a number average molecular weight of about 500–2,000 and are attached to linear segment by esterification of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Copy of International Search Report (PCT/US2004/003196) dated Jul. 16, 2004.
  • XP-002149703, Jun. 22, 1983, Derwent Publications Ltd., Abstract.