Abstract

A method for bending magnesium alloy tubes. The method includes heating the tube at moderate temperature in the range of about 100° C. to 200° C., and bending the tube to a bend angle or forming the tube to a desired shape.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 19.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for bending a magnesium alloy tube, the method comprising: heating the tube at a moderate temperature in the range of about 100° C. to 200° C.; and bending the tube to a bend angle, wherein said bending at said moderate temperature range provides a bend quality having one or more properties selected from the group consisting of: a maximum surface defect variance of less than or equal to about 5, a maximum % thinning variance of less than or equal to about 42, a standard deviation of % thinning of less than or equal to about 8.5, and combinations thereof.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein heating the tube comprises: heating a tooling; and holding the tube in the tooling until it is heated to the moderate temperature.

  3. Claim 3Depends on #1

    The method of claim 1 , further comprising placing the tube over a mandrel.