Abstract
A polyester resin prepared by polycondensing a dicarboxylic acid component containing terephthalic acid or derivative thereof with a diol component containing ethylene glycol through esterification or transesterification, thereby producing a melt polymerization polymer and subjecting the melt polymerization polymer to solid-phase polycondensation, wherein (1) the melt polymerization polymer contains comonomer units other than terephthalic acid units and ethylene glycol units in an amount of 5.5 or less, and whose intrinsic viscosity ranges from 0.08 dL/g to 0.50 dL/g and which has an apparent crystallite size smaller than 9 nm, and wherein (2) the melt polymerization polymer is subjected to solid-phase polycondensation at a temperature which is higher by at least 140° C. than the glass transition temperature of the melt polymerization polymer and is not higher than the melting point of the polymer to thereby obtain a polyester resin having an apparent crystallite size smaller than 9 nm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 5.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing a polyester resin, which comprises: polycondensing a dicarboxylic acid component containing terephthalic acid or an ester-forming derivative thereof as the main component and a diol component containing ethylene glycol as the main component, wherein the reacting components contain comonomers other than terephthalic acid and ethylene glycol in total amount of 5.5 mol % or less, by esterification or transesterification; melt polymerizing the polycondensed material obtained, thereby obtaining a polymerized product having an intrinsic viscosity ranging from 0.08 dL/g to 0.5
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗